Vehicular Accidents

Howell vs. Culbertson Stowers, Inc. (JOL260), investigation for attorney for the defendant of failure of weld on automobile axle housing.

Glascock vs. Pocahontas Ford & Mercury (JOK220), investigation for defendant attorney of failure of auto wheel studs and loss wheels..  

Elias vs. Swanson Auto Repair (JMJ170), investigation for plaintiff attorney of automobile frame straightening machine lift (jack) failure.

Estate of Blanc Cancio vs. Hyundai Motors (JLI250), consultant to attorney for plaintiff regarding collision involving a Hyundai automobile.

Michael Langston vs. Phillips Petroleum (JLB050), investigation for attorney for defendant for failure of vehicle axle resulting in van rollover.

Nowell vs. Ford (JKK250), consultant to attorney for the plaintiff regarding weld failure on brake pedal leading to automobile accident.

Cline Truck Accident (JKJ230), consultant to attorney for the plaintiff regarding weld failure on brake pedal leading to automobile accident.

Parnell Dodge Caravan Rollover (JJJ160), consultant to attorney for the plaintiff concerning rollover of a Dodge Caravan and axle failure.

Dykes vs. GESCO (JIE100), consultant to attorney for the defendant concerning failure of an automobile generator.

Orville Cumiford vs. GM, et al (JHE100), consultant to attorney for the plaintiff concerning failure of an automobile axle.

Robert Almand vs. So. Side Auto Parts (JGL310), consultant to attorney for plaintiff concerning failure of a high pressure hydraulic hose.

Cooper vs. General Motors (JCE220), consultant to attorney for the plaintiff concerning the sharpness of an automotive stamping.

Consultant to insurer of owner (JCD330) concerning failure of a Bronco axle.

Bludgett vs. APAC Caroline Inc. (JBB340), consultant to attorney for the plaintiff concerning failure of an automobile axle.

Keith vs. General Motors (JBB150), consultant to attorney for the plaintiff concerning an automobile axle failure.

Wampler vs. Radiator Specialty Co. (JAJ540), consultant to attorney for the defendant concerning design and material in automobile radiator.

Taylor vs. Ford Motor Co. (1981-10716), investigation for the attorney for the plaintiff of Thunderbird automobile transmission assembly.

Report to Hartford Insurance Group (1980-01001) concerning explosion during inflation of an aluminum automobile tire rim.

Report to attorney for the plaintiff (1980-00820) concerning failed seat bolt on 1974 BMW automobile.

Conally vs. Toyota Motor Sales (1978-80403), consultant to attorney for the defendant for evaluation of a Toyota automobile roof collapse.

Smith vs. Allied Supermarkets (1977-71208), consultant to attorney for the defendant concerning damage in a truck & automobile collision.

Report (1977-70911) to attorney for the plaintiff concerning the evaluation of a Mazda automobile seat frame failure.

Hayden vs. Ford Motor Co. (1976-61101), consultant to attorney for plaintiff concerning evaluation of a reported bearing failure.

Laughlin vs. Western Auto Supply Co., General Motors Corp., J.C. Penny Co., Inc., Kelly Springfield Tire Co. (1975-50602), consultant to attorney for the defendant concerning the evaluation of ball joint failure and tire blowout.

Oklahoma City vs. Boyes (1975-50401), consultant to attorney for the defendant concerning evaluation of abrasions on automobile trunk.

Cantwell and Rozell vs. Chrysler Corp. (1975-50205), consultant to attorney for the defendant for evaluation of wheel bearing failure.

LeMay vs. General Motors (J20838),. consultant to attorney for defendant concerning evaluation of a vehicle rollover and axle failure.

Kunkel vs. Bluebonnet (JUF160), investigation for attorney for plaintiff of wheels coming off rear tandem axle of tractor trailer and striking off-road pedestrian.

Porras Accident Investigation (JTF220), investigation of F-150 Ford truck wheel axle failure

Rost Litigation (JSA040), investigation for attorney for defendant of failure of a truck wheel axle and collision of wheel with vehicle..

Maine Fire Truck Fitting (JSA010), investigation of brass high pressure fitting failure and fatality.

Panhandle Trucking vs. Dave Roberts Leasing (JOA010), inspection for the plaintiff’s attorney of failure of truck steering gear.

Bryant vs. Rockwell (JIC040), consultant to attorney for the plaintiff concerning chipping from a truck axle.

Patterson vs. Maintain, Inc. (JHJ240), consultant to attorney for the defendant concerning failure of welded oilfield truck trailer hitch.

Beardsley vs. Rockwell Int. (JHF150), consultant to attorney for the plaintiff concerning chipping from a truck axle.

Jackson vs. AISD & General Motors (JHE140), consultant to attorney for the defendant concerning failure of leaf springs on school bus and disengagement of rear wheels and axle.

Layne vs. Bee Line (JGH230), consultant to attorney for the defendant concerning the design and failure of a shaft in a truck wheel alignment head.

Tate vs. Auto Convoy (JBL300), consultant to attorney for the defendant concerning accident involving auto transport carrier.

Consultant to owner (JBE150) concerning failure of a truck steering gear.

Keith vs. General Motors (JBB150), consultant to attorney for the plaintiff concerning a flying fragment from a truck axle.

Wilson vs. Bollinger (1981-J11251), investigation for the attorney for the defendant of accident involving defective truck trailer axle failure.

Flatt vs. Jackson (1980-004402),  consultant to Liberty Mutual Insurance Co. concerning failed welded truck trailer axle.

State of Ark. vs. Fuller (1980-00901), consultant to attorney for defendant of truck/automobile accident involving separation of welded truck axle.

Pearson vs. Litton Systems (1979-60802), consultant to attorney for the plaintiff concerning tractor trailer steering gear failure.

Hoffman vs. Cummings Engine (1977-71007), consultant to attorney for the plaintiff concerning the evaluation of truck engine bearing failure.

Carnes vs. Freightliner (1977-70403), consultant to attorney for the plaintiff for the evaluation of defective truck steering axle hub failure.

Hutchinson vs. Rockwell International (J41025), consultant to attorney for the plaintiff concerning a flying fragment from a truck axle.