During completion of an oil well, the casing string became stuck and unmovable. A dangerous and improper procedure was attempted in order to loosen and free the casing string. Power to the rotating string was reversed and the pipe was slowly turned three, one-quarter reverse turns. Unfortunately, the 1170° of reverse rotation still did not […]

The warm months are starting and we can finally get back to working outdoors in pleasantly beautiful spring-time weather. Many workers will cut some corners to try and make up for lost time over this seemingly endless winter. Cutting corners can cause injury and other costly damages. So this spring pay special attention to the […]

It was reported last week an oilfield rig exploded in West Texas killing three workers. The Upton County sheriff’s office said a well-servicing outfit was at the site when the explosion occurred Tuesday morning near Rankin, about 40 miles south of Midland. Officials did not release the names of those killed. Well owner Parsley Energy of […]

Contact Us

J.E.I. Metallurgical, Inc.

5514 Harbor Town
Dallas, Texas 75287

Phone: (972) 934-0493
Fax: (469) 737-3938
Email: r.c.jerner@metallurgist.com

Location Map

Follow Me On