Category: Wire Rope

During completion of an oil well, the casing string became stuck and unmovable. A dangerous and improper procedure was attempted in order to loosen and free the casing string. Power to the rotating string was reversed and the pipe was slowly turned three, one-quarter reverse turns. Unfortunately, the 1170° of reverse rotation still did not […]