Plastic Deformation

When the load causing a slight bed or stretch is removed, the component returns to its original shape/form. The metal has been subjected to elastic deformation. When the load exceeds the elastic limit and that load is now removed a permanent bend or deformation will persist. The metal is said to have become plastic. (See Bowing)