Taylor vs. Ford Motor Co. (1981-10716), investigation for the attorney for the plaintiff of Thunderbird automobile transmission assembly.

Laughlin vs. Western Auto Supply Co., General Motors Corp., J.C. Penny Co., Inc., Kelly Springfield Tire Co. (1975-50602), consultant to attorney for the defendant concerning the evaluation of ball joint failure and tire blowout.

Rost Litigation (JSA040), investigation for attorney for defendant of failure of a truck wheel axle and collision of wheel with vehicle.

Wampler vs. Radiator Specialty Co. (JAJ540), consultant to attorney for the defendant concerning design and material in automobile radiator.

Keith vs. General Motors (JBB150), consultant to attorney for the plaintiff concerning an automobile axle failure.

Bludgett vs. APAC Caroline Inc. (JBB340), consultant to attorney for the plaintiff concerning failure of an automobile axle.

Orville Cumiford vs. GM, et al (JHE100), consultant to attorney for the plaintiff concerning failure of an automobile axle.

Dykes vs. GESCO (JIE100), consultant to attorney for the defendant concerning failure of an automobile generator.

Cline Truck Accident (JKJ230), consultant to attorney for the plaintiff regarding weld failure on brake pedal leading to automobile accident.

Nowell vs. Ford (JKK250), consultant to attorney for the plaintiff regarding weld failure on brake pedal leading to automobile accident.

Estate of Blanc Cancio vs. Hyundi Motors (JLI250), consultant to attorney for plaintiff regarding collision involving a Hyundi automobile.

Elias vs. Swanson Auto Repair (JMJ170), investigation for plaintiff attorney of automobile frame straightening machine lift (jack) failure.

Howell vs. Culbertson Stowers, Inc. (JOL260), investigation for attorney for the defendant of failure of weld on automobile axle housing.

Oklahoma City vs. Boyes (1975-50401), consultant to attorney for the defendant concerning evaluation of abrasions on automobile trunk.

Report (1977-70911) to attorney for the plaintiff concerning the evaluation of a Mazda automobile seat frame failure.

Smith vs. Allied Supermarkets (1977-71208), consultant to attorney for the defendant concerning damage in a truck & automobile collision

Conally vs. Toyota Motor Sales (1978-80403), consultant to attorney for the defendant for evaluation of a Toyota automobile roof collapse.

Report to attorney for the plaintiff (1980-00820) concerning failed seat bolt on 1974 BMW automobile.

State of Ark. vs. Fuller (1980-00901), consultant to attorney for defendant of truck/automobile accident involving separation of welded truck axle.

Report to Hartford Insurance Group (1980-01001) concerning explosion during inflation of an aluminum automobile tire rim.

Tate vs. Auto Convoy (JBL300), consultant to attorney for the defendant concerning accident involving auto transport carrier.

Cooper vs. General Motors (JCE220), consultant to attorney for the plaintiff concerning the sharpness of an automotive stamping.

Gardner vs. Goodyear (JIJ210), consultant to attorney for the plaintiff concerning a vehicle falling from an elevated hydraulic automotive rack.

Elias vs. Swanson Auto Repair (JMJ170), investigation for plaintiff attorney of automobile frame straightening machine lift (jack) failure.

Glascock vs. Pocahontas Ford & Mercury (JOK220), investigation for defendant attorney of failure of auto wheel studs and loss wheels..    