Howell vs. Culbertson Stowers, Inc. (Jol260),
investigation for attorney for defendant of failure
of weld on automobile axle housing.
Rost Litigation (JSA040), investigation for attorney
for defendant of failure of a truck wheel axle and
collision of wheel with vehicle.
Porras Accident Investigation (JTF220),
investigation of F-150 Ford truck wheel axle
failure.
Kunkel vs. Bluebonnet (JUF160), investigation for
attorney for plaintiff of wheels coming off rear
tandem axle of tractor trailer and striking off-road
pedestrian.
Carnes vs. Freightliner (1977-70403), consultant to
attorney for the plaintiff for the evaluation of
defective truck steering axle hub failure.
Kibby vs. Williams (1980-00402), consultant to
attorney for plaintiff concerning evaluation of
accident involving 4-wheel drive front axle arm.
Flatt vs. Jackson (1980-004402), consultant to
Liberty Mutual Insurance Co. concerning failed
welded truck trailer axle.
State of Ark. vs. Fuller (1980-00901), consultant to
attorney for defendant of truck/automobile accident
involving separation of welded truck axle.
Wilson vs. Bollinger (1981-J11251), investigation
for the attorney for the defendant of accident
involving defective truck trailer axle failure.
LeMay vs. General Motors (J20838),. consultant to
attorney for defendant concerning evaluation of a
vehicle rollover and axle failure.
Hutchinson vs. Rockwell International (J41025),
consultant to attorney for the plaintiff concerning
a flying fragment from a truck axle.
Keith vs. General Motors (JBB150), consultant to
attorney for the plaintiff concerning a flying
fragment from a truck axle.
Bludgett vs. APAC Caroline Inc. (JBB340), consultant
to attorney for the plaintiff concerning failure of
an automobile axle.
Consultant to insurer of owner (JCD330) concerning
failure of a Bronco axle.
Orville Cumiford vs. GM, et al (JHE100), consultant
to attorney for the plaintiff concerning failure of
an automobile axle.
Jackson vs. AISD & General Motors (JHE140),
consultant to attorney for the defendant concerning
failure of leaf springs on school bus and
disengagement of rear wheels and axle.
Beardsley vs. Rockwell Int. (JHF150), consultant to
attorney for the plaintiff concerning chipping from
a truck axle.
Bryant vs. Rockwell (JIC040), consultant to attorney
for the plaintiff concerning chipping from a truck
axle.
Parnell Dodge Caravan Rollover (JJJ160), consultant
to attorney for the plaintiff concerning rollover of
a Dodge Caravan and axle failure.
Michael Langston vs. Phillips Petroleum (JLB050),
investigation for attorney for defendant for failure
of vehicle axle resulting in van rollover.