Equipment - Oil Field
Lamb vs. Acme Tool (1974-40402), consultant to
attorney for plaintiff concerning the failure of
down-hole oil well equipment.
Report (1974-41002) to Kerr-McGee concerning
evaluation of failed pipe in oil collecting system.
Report (1975-51202) to Chevron Oil Co. concerning
evaluation of a drill pipe failure.
Hess Oil Virgin Island Corp. vs. Ward Industries
Pipe Fabricating (1976-60603), consultant to
attorney for the defendant concerning welded piping
component failure in refinery explosion fire.
Report (1977-704012) to attorney for defendant
concerning the evaluation of high pressure mud
system oil field fittings.
Fields vs. American Hoist & Derrick (1977-71012),
consultant to attorney for the defendant for the
evaluation of oilfield drilling derrick collapse.
Loomis vs. American Hoist & Derrick (1978-80102),
consultant to attorney for the defendant for
evaluation of oilfield rat hole rig brake failure.
Pride Oilfield Services, Inc. (1981-10729),
investigation and report concerning the collapse of
drilling rig.
Cameron Iron Works vs. Quality Oilfield Products
(JEJ310), consultant to attorney for the defendant
concerning alleged patent infringement.
Patterson vs. Maintain, Inc. (JHJ240), consultant to
attorney for the defendant concerning failure of
welded oilfield truck trailer hitch.
Kirby vs. Patterson Energy (JME060), investigation
for attorney for defendant of oilfield drilling rig
collapse.
Richard A. McDonald vs. Oilfield Pro Log Services,
Inc. (JOA020), evaluation for plaintiff's attorney
of oil well metal and tool samples.
Fuentes & Seigiera vs. McGuire Industries, et al
(JLB020) investigation for attorney for defendant of
failure of oil field equipment.
Sherry vs. Wellmark & Natco (JLD120), investigation
for attorney for defendant of failure of fitting on
oilfield pressure vessel during hydro testing.
Report (1974-41105) to Farmer's Insurance concerning
evaluation of broken lifting hook from oilfield
equipment.
Mills vs. Crane Carrier Corp. (1978-80202),
consultant to attorney for the defendant for the
evaluation of an oilfield drilling mast collapse.
Stephenson/Taylor Estate vs. RHS (JHL320),
consultant to attorney for the defendant concerning
failure of oil field hydraulic pulling jack.
Oxley vs. Picoma Industries (JIA010), consultant to
attorney for the defendant concerning failure of
oilfield casing couplings.
Delacerda vs. McKissic-Crosby Croup, Inc. (JJJ190),
investigation for attorney for plaintiff of door on
oilfield drilling rig casting failure which resulted
in head injury.
Doyon Drilling Sling Failure (JKG140), consultant to
company on failure of an oilfield tubular goods
lifting sling.
Fuentes & Seigiera vs. McGuire Industries, et al
(JLB020) investigation for attorney for defendant of
failure of oilfield equipment.
Back to Forensic Investigations
|