Equipment Pipeline

Equipment - Pipelines

Richard Hall vs. Ashland Oil Company (J30516), consultant to attorney for defendant, about failure of a pipeline used to transmit chlorine gas.

Consultant to Eby Construction, Witchita, Kansas (JAG090) concerning alleged defective welding in a water pipeline.

Hatto vs. NW Central Pipeline (JBG370), consultant to attorney for the defendant concerning front end loader penetration of high pressure gas transmission line and resulting explosion/fire.

ANR Pipeline vs. Okemah Construction (JDA410), consultant to insurer of the defendant on physical damage to a pipeline.

Consultant to U.S. Ary Corp. of Engineers (88I22I) concerning failure and testing of welded stainless steel pipeline.

Mapco vs. Flint (JIH180), consultant to attorney for the defendant concerning failure of a welded ammonia pipeline.

Vieregge vs. Lone Star Steel (JJI150), consultant to the defendant concerning failure of a gasoline pipeline.

Fallwell vs. Norpan Corp. (JJJ200), consultant to attorney for defendant of flash fire burn through stainless steel pipeline in oxygen letdown station.

KN Pipeline Rupture (JNE160), assessment of cause of pipeline failure.

Perkins vs. Entergy Corp. (JNK310), investigation for attorney for the defendant of failure, fire of hydrogen gas pipeline and valve assembly.

Genesis Crude Oil Pipeline Failure (JOL280), investigation of failure of crude oil pipeline.

McClure vs. City of Seminole (1974-41104), consultant to attorney for plaintiff concerning evaluation of gas pipeline failure and explosion.

Filson vs. Phillips Petroleum Co. (1976-60902), consultant to attorney for the plaintiff concerning evaluation of gas pipeline corrosion.

Aminoil-Lucian Pipeline (1977-71005), consultant to the defendant concerning the evaluation of a PVC plastic pipeline failure and explosion.

Bird Oil Equity of OK Ltd. vs. Richard Long (1978-80101), Consultant for attorney to the plaintiff for the evaluation of gas pipeline corrosion.

Anadarko Const. vs. Aminoil (1978-80306), consultant to attorney for defendant concerning failure in PVC plastic gas pipeline explosion.

Mustang Fuel vs. Youngstown Sheet and Tube (1978-80611), consultant to attorney for the defendant concerning gas pipeline explosion.

M. Lewis vs. Transok Pipeline (1978-81107), consultant to attorney for plaintiff in explosion of 6 inch bolted cover of an oil and gas pipeline valve.