Equipment Shafts

Failure Mode - Corrosion

AC/DC Partnership vs. Ohio Casualty Ins. (JML230); investigation for plaintiff of corrosion from chlorine spill, hydrochloric acid formation.

Duncan Properties Tubing Corrosion (JNC080), investigation of down-hole corrosion failure of tubing in McMakin #1, Washita County, OK.

Ice Group Addison vs. C.W. Davis Supply, Chill-Con Products, Ltd. (JNE190), investigation of corrosion failure of heat exchanger tubes

Beck Plumbing Leak (JSB060), investigation of copper water pipe corrosion and electrical arcing.

CMD Realty Water Line Failure (JTC130), investigation of corrosion of 10 inch cooling water line.

Filson vs. Phillips Petroleum Co. (1976-60902), consultant to attorney for the plaintiff concerning evaluation of gas pipeline corrosion.

Bodard & Hale Drilling vs. Wheeling Pittsburgh Steel (1977-70409), consultant to attorney for the defendant of drill pipe corrosion fatigue problem.

Bird Oil Equity of OK Ltd. vs. Richard Long (1978-80101), consultant for attorney to the plaintiff for the evaluation of gas pipeline corrosion.

Schick Oil & Gas (J20639), consultant to plaintiff for identification of 1200 feet of 2-7/8" tubing and type of corrosion.

Report to Howard Thronhill, Midstates Analytical Laboratories (J20930) of Inconel sheath corrosion.

Midland Water Treatment Plant (JGA040), consultant to company concerning corrosion from inadequate undercoating/painting.

Johnson vs. Lone Star Gas (JGB090), consultant to attorney for plaintiff concerning coupling pipe corrosion and subsequent house explosion.

Bill's Auto Parts Loss (JGE110), consultant to attorney for the defendant for evaluation of alleged corrosion resulting from water damage.

Resource Trailer vs. Fisher (JGL320), consultant for the defendant concerning effect of cargo on corrosion in truck trailers.

Nichols & Stanley vs. Georgia Pacific (JIF130), consultant to attorney for the plaintiff concerning corrosion and failure of welded overhead walkway.

Tulsa School Board Goal Failure (JIJ240), consultant to attorney for the school board concerning corrosion and adequacy of welded soccer goal.

Horner Food vs. AAA Refrigeration (JIK260), consultant to attorney for the defendant concerning corrosion due to placement of a refrigerant line.

 