Failure Mode - Fire
Report to Universal Claims (1975-50403) concerning
evaluation of explosion and mobile home fire.
Report (1975-50801) to Universal Claims concerning
evaluation of explosion and residential fire at
Poteau, Oklahoma.
Hess Oil Virgin Island Corp. vs. Ward Industries
Pipe Fabricating (1976-60603), consultant to
attorney for the defendant concerning welded piping
component failure in refinery explosion fire.
Report (1977-71108) to attorney for the defendant
concerning the evaluation of metal sparking and
gasoline fire/explosion.
Henkelman vs. Airco (1978-80901), consultant to
attorney for the defendant concerning a fire and
explosion involving liquid oxygen pump.
Investigation and analysis of fire damage to
drilling rig substructure for Universal Resources
Corp., (1981-10701).
E & M Machine Shop vs. Brown Welding Supply
(1981-10717), investigation for attorney for the
plaintiff of acetylene tank explosion and fire.
Cactus Feeders & Ranger Ins. vs. WEMCON Corp.
(J20235), investigation for the attorney for
defendant of explosion and fire in a cattle feedlot.
Frank Yancy vs. Big Three Industries (J20632),
consultant to defendant concerning cause of an
acetylene tank rupture and subsequent fire.
Lonnie Northcliff vs. Bennett & Harris Propane
(J21035), consultant to attorney for defendant of
failure of gas fitting and fire.
Consultant to insurer of Brentwood Forrest
Apartments (J30517) concerning flexible gas line
failure and its relationship to apartment fire.
Consultant to Owner's insurance company (J30813)
concerning fire damage evaluation on a gooseneck
trailer.
American Enterprises vs. White Motor & General
Motors Corp. (J31001), consultant to attorney for
the plaintiff of fire damage to a garbage truck
starter solenoid.
Consultant to attorney for defendant, Fairchild
Industries, Inc. (J31038), concerning in-flight fire
on Air-Canada DC-9 crash.
Consultant to insurer of coal company scraper
(J40410) concerning the evaluation of fire damage to
a scraper/tractor frame.
Sledge Welding vs. General Processing (JBA600),
consultant to attorney for the defendant concerning
an acetylene cylinder fire.
Consultant to insurer of owner (JBJ110) concerning a
weld failure in a hot oil pumper unit and subsequent
fire/explosion.
Report (JDK823) to Exxon Corp. concerning explosion
and fire in tertiary oil recovery operation.
Thompson vs. Federal Pacific Electric (JEA020),
consultant to attorney for the defendant concerning
failure of electrical switch and fire.
Britt vs. S.E. Air Gas (JFJ200), consultant to
attorney for the defendant concerning fire/explosion
sequence and integrity of fusible plug.
Aston vs. SPS (JID080), consultant to attorney for
the defendant concerning a range fire due to arcing
from a high voltage electric line.
Beavers vs. Sisson (JID090), consultant to attorney
for the defendant concerning failure of a gas line
valve and propane/butane explosion/fire.
1st Methodist vs. Whittaker, d/b/a Quality Air,
(JKD090), consultant to attorney for the defendant
concerning furnace involved in fire.
Davis vs. Sloan (JKI180), consultant to attorney for
the defendant concerning a piping failure resulting
in a propane fire/explosion.
McGee vs. Elmwood Sensors (JKJ220), consultant to
attorney for the defendant of failure of an
electrical switch in a deep fryer resulting in a
fire.
Perkins vs. Air Liquide (JKI200), consultant to
attorney for the defendant of flash fire burn
through stainless steel pipeline in oxygen letdown
station.
Hugh Porter vs. Majestic Co. & Eastbrook Builders
(JLE140), investigation for attorney of defendant of
metallurgical evidence in a chimney fire.
What-a-Burger vs. Pitco (JLI210), consultant to
attorney for the defendant of fire which originated
at deep-fry unit of house fan bracket failure.
Deaf Smith Co. Grain Processor vs. Springer Electric
Coop (JMF100), investigation for attorney for
plaintiff of wire splice failure & high voltage
fire.
Dahais Food Stores Inc. vs. Valmont Electric
(JNI260), evaluation of fire.
Wicker 1998 Western Star Fire (JOA030),
investigation of burned tractor.
Malden Mills vs. Rhone-Poulene (JPB070),
investigation for attorney for the defendant of pipe
and boiler components in a textile mill fire.