Public Leasing
Corporation vs. Mack Truck International
(1971), consultant to attorney for
plaintiff concerning casting failures.
Archer vs. Elliot Manufacturing (1972),
consultant to attorney for plaintiff
concerning hydraulic cylinder weld
failure.
R.L. Keown vs. King Seely (1972),
consultant to attorney for plaintiff
concerning defective lantern valve.
Gravitt vs. Chrysler Corporation (1972),
consultant to attorney for plaintiff
concerning steering gear failure.
Crittenden vs. Kent-Moore Tool (1972),
consultant to attorney for plaintiff
concerning spalling of staking tool.
Report (1972) to St. Paul Insurance
Company concerning evaluation of armored
car wheel lug fatigue failure.
L.D. Boyd vs. International Harvester
(1972), consultant to attorney for
plaintiff concerning evaluation of king
pin failure.
Jerry Reams vs. Plumb Company (1972),
consultant to attorney for plaintiff
concerning spalling from the head of
claw hammer.
J.L. Norton vs. Cotton Electric
Corporation (1972), consultant to
attorney for defendant concerning
transmission line pole insulator tie
failure.
Rouse vs. International Harvester (1972)
consultant to attorney for plaintiff
concerning king pin failure.
Capshaw vs. Westinghouse Air Brake
(1972-213), consultant to attorney for
plaintiff concerning earth mover axle
failure.
Kilgore vs. General Fire Extinguisher
(1972-214), consultant to attorney for
defendant concerning corrosion
evaluation.
Report (1972) to St. Paul Insurance
Company concerning evaluation of motor
boat steering bolt fatigue failure.
Pittinger vs. Hearn (1972), consultant
to attorney for defendant concerning
evaluation of sintered brass products.
Home Insurance Company vs. William
Automatic Sprinkler (1972), consultant
to attorney for plaintiff concerning
failure of check valve.
Turner vs. Toyota Motor Car (1972-218),
consultant to attorney for plaintiff
concerning rear axle failure.
Cimarron Industries vs. Public Leasing
Corporation (1973), consultant to
attorney for the plaintiff concerning
failure of defective aluminum castings.
Investigation (1973), for Royal Globe
Insurance Company concerning evaluation
of truck frame failure.
A. C. Hoyle vs. Superior Welding, Inc.
(1973), consultant to attorney for
plaintiff concerning failure of welded
structure.
Drewery vs. Rockwell Manufacturing
(1973), consultant to attorney for
defendant concerning evaluation of truck
spring failure.
Benna vs. Page Airmotive (1973-305),
consultant to attorney for defendant
concerning evaluation of aircraft engine
failure.
Meyer vs. Freightliner (1973-306),
consultant to attorney for defendant
concerning evaluation of truck radius
rod failure.
U.S. Mags vs. Home Indemnity (1973-308),
consultant to Middlesex Mutual Ins. Co.
concerning evaluation of magnesium rim
failure.
Martin Sprocket and McDonald vs. Gear
(1973), consultant to attorney for
defendant concerning evaluation of gear
failure.
Price vs. Utilities Equipment
(1973-310), consultant to attorney for
defendant concerning evaluation of
hydraulic cylinder failure.
Casteel vs. Sooner Supply (1973-311),
consultant to attorney for defendant in
investigation of oxygen cylinder
explosion.
Nolen vs. Taylor Chain (1973),
consultant to attorney for defendant
concerning question of defectively
welded chain.
Associated Aviation vs. Lycoming (1974),
consultant to attorney for plaintiff for
evaluation of failure of aircraft
engine.
Banks vs. General Motors (1974-40304),
consultant to attorney for plaintiff
concerning evaluation of truck spring
failure.
Report (1974) to Associated Aviation
Underwriters for evaluation of failed
aircraft landing gear housing.
Merrill vs. McKaig (1974), consultant to
Employer's Casualty Company for
evaluation of truck tie rod failure.
Fanning vs. Sears (1974-40502),
consultant to attorney for plaintiff
for evaluation of chipping failure from
a punch.
Keen vs. United States (1974-40503),
consultant to attorney for plaintiff for
evaluation of jet engine failure.
Santa Fe Railroad vs. Gulf Insurance
(1974-40601), consultant to attorney for
defendant for evaluation of train
derailment.
Roos vs. Werner Ladder Company (1974),
consultant to attorney for defendant
of a failure in a stepladder.
Woodall vs. Honda (1974-40701),
consultant to attorney for defendant
concerning evaluation of failed
motorcycle part.
Giles vs. City Springs (1974-40801),
consultant to attorney for defendant of
broken "Shur Guide" and wrecked truck.
Lamb vs. Acme Tool (1974-40402),
consultant to attorney for plaintiff of
the failure of down-hole oil well
equipment.
Brock vs. Ellex Transport Co.
(1974-40805), consultant to defendant
for evaluation of truck fifth wheel
failure.
Guthrie vs. Vendo Machine (1974-40807),
consultant to attorney for plaintiff of
vending machine hinge fatigue failure.
Abbott vs. Coca-Cola (1974-40901),
consultant to attorney for plaintiff
concerning fatigue in a plastic Coke
carton failure.
Report (1974-41001) to Tulsa Produce
Company concerning natural gas
explosion.
Report (1974-41002) to Kerr-McGee
concerning failed pipe in oil collecting
system.
McClure vs. City of Seminole
(1974-41104), consultant to attorney for
plaintiff for evaluation of gas pipeline
failure and explosion.
Lee vs. Continental Can (1974-41103),
consultant to attorney for defendant for
evaluation of explosive failure of block
sealer containers.
Report (1974-41105) to Farmer's
Insurance for evaluation of broken
lifting hook from oil field equipment.
Report (1974-41108) to Alliance
Insurance for evaluation of defective
gasoline pump valve and explosion.
Report (1974-41109) to Claims Management
Corporation for evaluation of explosion
of natural gas engine cover plate.
Jones vs. Freightliner (1974-41201),
consultant to attorney for plaintiff
concerning evaluation of failed truck
wheel.
Bridges vs. Enterpoint Corp.
(1975-50101), consultant to Hartford
Insurance Company for evaluation of
truck wheel lug failures.
Report (1975-50102) to Universal Claims
Service for evaluation of failed bus
leaf spring.
Yon vs. Winchester (1975-50103),
consultant to attorney for plaintiff
for evaluation of shotgun.
Report (1975-50201) to The Hanover
Insurance Company for evaluation of
water tank explosion.
Report (1975-50204) to Transport
Indemnity for the evaluation of a truck
steering kingpin failure on Bekins
moving van.
Hulsey vs. 7-Up Bottling Co. of Oklahoma
City (1975-50601), consultant for
defendant for evaluation of a truck
brake line failure.
Sebald vs. Bell Helicopter & Allison
Division of General Motors Corporation
(1975-50704), consultant to attorney for
plaintiff concerning jet engine blade
failure.
LaCoste, Lovett vs. Allegheny Ludlum
Steel Corp. (1975-50905), consultant to
attorney for defendant of Chinook
helicopter combining transmission spiral
bevel gear failure.
Pollard vs. McDonough (1975-50202),
consultant to attorney for plaintiff
concerning spalling/chipping from hammer
and ax.
Cantwell and Rozell vs. Chrysler Corp.
(1975-50205), consultant to attorney for
defendant for evaluation of wheel
bearing failure.
Taylor vs. Heller Tool Co. (1975-50206),
consultant to attorney for defendant
concerning evaluation of hammer failure.
Oklahoma City vs. Boyes (1975-50401),
consultant to attorney for defendant
concerning evaluation of abrasions on
automobile trunk.
Report to Universal Claims (1975-50403)
concerning evaluation of explosion and
mobile home fire.
Laughlin vs. Western Auto Supply Co.,
General Motors Corp., J.C. Penney Co.,
Inc., Kelly Springfield Tire Co.
(1975-50602), consultant to attorney for
defendant concerning the evaluation of
ball joint failure and tire blowout.
Keith vs. Childress Oil Co.
(1975-50703), consultant for plaintiff
concerning evaluation of truck
distributor cap debris.
Report (1975-50801) to Universal Claims
concerning evaluation of explosion and
residential fire at Poteau, Oklahoma.
Report (1975-50802) to attorney for
defendant concerning evaluation of
failure of supports for welded stool
chair seat.
Corbett vs. Sears Roebuck & Co. &
Western Forge Corp. (1975-50806),
consultant to attorney for plaintiff
concerning drive pin chipping failure.
Report (1975-51007) to Accident
Reconstruction Lab, Dallas, TX for the
evaluation of a truck fifth wheel welded
bracket failure.
Hall vs. Big Three Industries
(1975-50906), consultant to attorney for defendant concerning an acetylene
cylinder failure/explosion.
Burks vs. Freightliner Corp.
(1975-51005), consultant to attorney for
plaintiff concerning the evaluation of
truck engine mount failure.
England vs. American Gauge (1975-51001),
consultant to attorney for plaintiff of
forging deficiency in portable fence
stretcher/come-along.
Wilson vs. Sears Roebuck & Co.
(1975-51002), consultant to attorney for
plaintiff concerning defective drive pin
punch chipping failure.
Grego vs. General Motors (1975-51003),
consultant to attorney for plaintiff
concerning evaluation of bumper jack
failure.
Conner vs. Winchester Arms (1975-51209),
consultant to attorney for plaintiff of
a shotgun hammer & trigger assembly
material and heat treatment.
Report (1975-51202) to Chevron Oil Co.
concerning evaluation of a drill pipe
failure.
Report (1975-51206) to Askew Associates,
Inc. concerning evaluation of prop
failure.
Miles vs. Bell Helicopter (1976-60301),
consultant to plaintiff concerning the
evaluation of aluminum helicopter
push-pull tube.
Miller vs. Pioneer Gas (1976-60203),
consultant to attorneys for defendant
concerning evaluation of oxygen cylinder
explosion.
Edmonson vs. Bell Helicopter Corp.
(1976-60205), investigation for attorney
for plaintiff of failed spherical spine
from coupling on helicopter.
Oxley vs. Big Chief (1976), consultant
to attorney for plaintiff concerning
evaluation of a drill pipe failure.
Smedley vs. Waco of Oklahoma
(1976-60302), consultant to attorney for
defendant concerning a powered
scaffolding system failure.
Watts vs. Ridge Tool Co. (1976),
consultant to attorney for plaintiff
concerning evaluation of a pipe wrench
failure.
Oklahoma Flower Market vs. Scott
Chevrolet (1976-60307), consultant to
Employer's Casualty Co. for the
evaluation of truck brake line failure.
Simon vs. Land and Marine Rental Co.
(1976), consultant to attorney for
plaintiff concerning the evaluation of a
drill pipe failure.
Dyco Petroleum Corp. vs. The Rucker Co.
(1976-60504), consultant to attorney for
the plaintiff for the evaluation of a
drill pipe failure.
Shelton vs. Remington Arms (1976-60505),
consultant to attorney for defendant
concerning the evaluation of a shotgun
explosion.
Lyles vs. American Hoist and Derrick
(1976-60506), consultant to attorney for
defendant concerning evaluation of steel
cable failure.
Dearmore vs. Montgomery Ward
(1976-60507), consultant to attorney for
defendant concerning air compressor tank
failure and explosion.
Hess Oil Virgin Island Corp. vs. Ward
Industries Pipe Fabricating
(1976-60603), consultant to attorney for
defendant concerning welded piping
component failure in refinery
explosion/fire.
Turpin vs. Ford Motor Co. (1976-60604),
consultant to attorney for plaintiff
concerning evaluation of a truck
steering linkage failure.
Schoonover vs. International Harvester
(1976-60802), consultant to attorney for
the plaintiff concerning tractor trailer
steering gear failure.
Hein vs. Brown Stove Works, Inc.
(1976-60803), consultant to attorney for
defendant concerning aluminum tube
failure in gas cooking stove.
Filson vs. Phillips Petroleum Co.
(1976-60902), consultant to attorney for
plaintiff concerning evaluation of gas
pipeline corrosion.
American Hotels vs. Big Three Industries
(1976-60904), consultant to attorney for
defendant concerning acetylene cylinder
explosion.
Report (1976-61102) to Hanover Insurance
Co. concerning hoop rod failures in
collapse of silo in the matter of Weir
vs. Southwestern Silo.
S.A.R. Water Corp. vs. Phillips
Petroleum Co. (1976-61005), consultant
to attorney for plaintiff concerning
plastic pipe joint failures.
Hayden vs. Ford Motor Co. (1976-61101),
consultant to attorney for plaintiff
concerning evaluation of bearing
failure.
Hall vs. Browning Arms (1976-61104),
consultant to attorney for defendant
concerning evaluation of bicycle rim
weld failure.
Johnson vs. Alan Bradley (1976-61202),
consultant to attorney for defendant
concerning plastic phenolic electrical
switch failure.
Report (1977-70201) to General
Adjustment Bureau concerning the
evaluation of welded truck spring
bracket failure.
Eaglebarger vs. Harley Davidson Motor
Company (1977-70302), consultant to
attorney for defendant concerning
motorcycle spoke failure.
Report (1977-70105) to MFA Insurance
concerning dislodgement of diamond from
ring mounting.
Report to attorney for the plaintiff
(1977-70307) concerning the evaluation
of a chair weld failure.
Carnes vs. Freightliner (1977-70403),
consultant to attorney for plaintiff for
tevaluation of defective truck steering
axle hub failure.
Hawkins vs. Otasco (1977-70408),
consultant to CNA Insurance concerning
the evaluation of magnesium wheel
failure.
Bodard & Hale Drilling vs. Wheeling
Pittsburgh Steel (1977-70409),
consultant to attorney for defendant of
drill pipe corrosion fatigue problem.
Shumacher vs. Mitsubishi (1977),
consultant to attorney for the defendant
for the evaluation of the cause for the
loss of MU-2 Aircraft.
Report (1977-704012) to attorney for
defendant concerning the evaluation of
high pressure mud system oil field
fittings.
Mantone vs. Fruehauf (1977-70501),
consultant to attorney for defendant
concerning the evaluation of a truck
accident.
Report (1977-70607) to Liberty Mutual
Insurance concerning the evaluation of a
grinding disc failure.
Blehm vs. Floyd's Campers (1977-70608),
consultant to attorney for defendant
concerning the evaluation of a camper
jack failure.
Monk vs. Fruehauf (1977-70705),
consultant to attorney for defendant
concerning evaluation of collapsed truck
trailer wheel jack.
Saurbry vs. Arden Drilling (1977-70706),
consultant to attorney for plaintiff
concerning the evaluation of lifting eye
failure.
Inexco vs. Shebester of Hennessey
(1977-70707), consultant to attorney for
defendant concerning evaluation of slip
damaged drill pipe.
King vs. White Freightliner
(1977-70709), consultant to attorney for
plaintiff concerning the evaluation of
truck brake failure.
Babcock vs. Hertz (1977-70710),
consultant to attorney for defendant
concerning evaluation of truck brake
failure.
Report (1977-70711) to Acme-Rucker
concerning the evaluation of a drill
pipe washout.
Report (1977-70712) to Acme-Rucker
concerning the evaluation of a
longitudinal drill pipe split.
Report (1977-70800) to attorney for
plaintiff concerning the evaluation of a
tie rod failure.
Kidd vs. O'Neal Tank Company
(1977-70806), consultant to attorney for
the defendant concerning the evaluation
of a valve failure.
Report (1977-70908) concerning the
evaluation of a hydraulic truck bed
hoist weld failure.
Report (1977-70911) to attorney for the
plaintiff concerning evaluation of a
Mazda automobile seat frame failure.
Aminoil-Lucian Pipeline (1977-71005),
consultant to defendant concerning
evaluation of a PVC plastic pipeline
failure and explosion.
Mitchell vs. Hughes Aircraft
(1977-71006), consultant to attorney for
plaintiff for evaluation of helicopter
rear rotor bolt failure.
Hoffman vs. Cummings Engine
(1977-71007), consultant to attorney for
plaintiff concerning evaluation of truck
engine bearing failure.
Harlow vs. Kinetics (1977-71009),
consultant to attorney for plaintiff for
evaluation of fiberglass plastic gas
transmission pipe failure.
Fields vs. American Hoist & Derrick
(1977-71012), consultant to attorney for
defendant for evaluation of oilfield
drilling derrick collapse.
Johnson vs. Walker-Neer Mfg.
(1977-71106), consultant to attorney for
defendant concerning evaluation of
drilling rig collapse.
Wilson vs. Kawasaki (1977-71107),
consultant to attorney for defendant
concerning evaluation of motorcycle
spoke and tire failure.
Report (1977-71108) to attorney for
defendant concerning evaluation of metal
sparking and gasoline fire/explosion.
Ludtke vs. Otasco (1977-71115),
consultant to attorney for defendant
concerning evaluation of a hammer chip.
Rosebrough vs. Eureka Water Co.
(1977-71207), investigation for attorney
for defendant concerning glass water
bottle explosion.
Smith vs. Allied Supermarkets
(1977-71208), consultant to attorney for
defendant concerning damage in a truck
and automobile collision.
Brennan vs. Teledyne Wisconsin Motors
(1977-71210), consultant to attorney for
defendant concerning flywheel
disintegration.
Bird Oil Equity of OK Ltd. vs. Richard
Long (1978-80101), consultant for
attorney for plaintiff for evaluation of
gas pipeline corrosion.
Loomis vs. American Hoist & Derrick
(1978-80102), consultant to attorney for
defendant for evaluation of oilfield rat
hole rig brake failure.
Report (1978-80107) to The Hartford
Insurance Co. concerning hydraulic
lifting mechanism failure.
Chubb and Son vs. Ford Motor Co.
(1978-80110), consultant to attorney for
plaintiff concerning truck spring center
bolt in truck accident.
Report (1978-80113) to Oklahoma Farmers
Union concerning the evaluation of
Stevens’s shotgun explosion.
Mills vs. Crane Carrier Corp.
(1978-80202), consultant to attorney for
defendant for evaluation of oilfield
drilling mast collapse.
Ralston Oil and Gas Company vs. Genesco
Inc. (1978-80301), consultant to
attorney for plaintiff concerning ERW
welded pipe failure.
Burrell vs. Grozier-Mann Oil Company
(1978-80305), consultant to attorney for
plaintiff concerning evaluation of truck
lug failure.
Anadarko Const. vs. Aminoil
(1978-80306), consultant to attorney for
defendant concerning failure in PVC
plastic gas pipeline explosion.
Ferguson vs. Garrett Research & Rockwell
International (1978-80307), consultant
to attorney for defendant of an aircraft
mid-air disintegration.
Metalsource Corp. vs. Dallas
International Bank vs. Land-Air, Inc. &
Gus Bowman (1978-80313), consultant to
attorney for plaintiff concerning
evaluation of steel bomb lug forging
defects.
Connally vs. Toyota Motor Sales
(1978-80403), consultant to attorney for defendant for evaluation of a Toyota
automobile roof collapse.
Moore vs. Gibson Discount Center
(1978-80404), consultant to attorney for
plaintiff concerning evaluation of Freon
can explosion.
West Friona Grain vs. Allied Millwright
(1978-80408), consultant to attorney for
defendant for evaluation of evidence
from silo explosion.
Emile P. Vead vs. Halliburton
(1978-80602), consultant to attorney for
defendant concerning evidence in
off-shore oil drilling rig accident.
Report (1978-80605) to The Hartford
Group for the defendant concerning
evaluation of truck tire ring failure.
Mustang Fuel vs. Youngstown Sheet and
Tube (1978-80611),consultant to attorney
for defendant concerning gas pipeline
explosion.
Stacy vs. Cessna & Tulsa Lease-A-Plane
(1978-80615), consultant to attorney for
defendant of Cessna 210 aircraft crash.
Ramos vs. Union (1978-80616), consultant
to attorney for defendant concerning
evaluation of a serving machine
accident.
Stanley Lawson vs. Willis Wells
(1978-80701), consultant to attorney for
plaintiff concerning circumstances
surrounding boat accident.
Report to attorney for plaintiff
(1978-80803), concerning examination of
Hornet ignition system and its
relationship to one vehicle accident.
Consultant to attorney for plaintiff
(1978-80806) concerning investigation of
Hughes helicopter crash.
Henkelman vs. Airco (1978-80901),
consultant to attorney for defendant
concerning fire and explosion involving
liquid oxygen pump.
Wilkson vs. Ford Motor Co. (1978-80905),
consultant to attorney for plaintiff
concerning accident involving 1977 Ford
Landau vehicle.
Report to attorney for the plaintiff
(1978-81003) concerning fractured
torsion bar support bracket from wrecked
1973 Kenworth K100 truck.
Report to Hartford Insurance Group
(1978-81019) concerning Dohrn
International Truck wreckage
examination.
Report to Hartford Insurance Group
(1978-81020) concerning investigation of
a concrete saw and causes of saw blade
disintegration.
Report to Hartford Insurance Group
(1978-81022) concerning failure of
fractured 2-5/16 inch trailer ball.
M. Lewis vs. Transok Pipeline
(1978-81107), consultant to attorney for
plaintiff in explosion of 6 inch bolted
cover of an oil and gas pipeline valve.
Tripp vs. Rego (1978-81111), consultant
to attorney for defendant in explosion
of a liquid propane gas tank.
Kinetics vs. El Paso Products, Inc.
(1978-81113), consultant to attorney
forplaintiff and materials evaluation of
reinforced resin line pipe.
Taylor vs. Piper (1978-81115),
consultant to attorney for defendant and
metallurgical analysis of wrecked Piper
Comanche aircraft.
Report to Kirby Exploration Co.
(1978-81203) concerning metallurgical
and failure analysis of failed
non-rotating polishing mandrel.
Jackson vs. Fletcher (1978-81210),
consultant to plaintiff concerning
investigation of wrecked 1977
International tractor trailer.
Examination of Maverick Head Lamps
(1979-90101), consultant to insurance
adjusters for evaluation of light bulb
condition during collision.
Report to CNA Insurance (1979-90103)
concerning examination of Peterbilt
truck diesel engine rods.
Consultant to the defendant (1979-90207)
concerning examination of metallurgical
failure at Public Service Company power
plant in Oklahoma.
Report to UEC Manufacturing Company
(1979-J90306) regarding failure analysis
of UEC skyjacker welded bracket.
Pearson vs. Litton Systems (1979-90321),
consultant to attorney for defendant
concerning transmission gear failure and
helicopter crash.
Headlamp Inspection (1979-90401),
consultant to attorney for defendant for
exam of motorcycle headlamp condition at
time of impact.
Utzman vs. Bethany Boat (1979-90403),
consultant to attorney for plaintiff
concerning boat trailer separation and
impact with oncoming vehicle.
Report concerning analysis of babbitt
bearing failures occurring at gas
processing plant (1979-90405).
Report to Underwriter's Adjusting Co.
(1979-90406) concerning examination of
failed truck trailer leaf spring from
pipe supply inspection trailer.
Report to Moran Brothers Energy, Inc.
(1979-90407) concerning failure analysis
of 5-inch Grade E drill pipe.
Phillips & Linder vs. Teledyne
Continental Engine (1979-90412),
consultant to attorney fordefendant
concerning examination of aircraft
engine cylinder flange hold-down studs.
Consultant to USF&G (1979-90501) for
Craftsman drive pin punch involved in
industrial accident resulting in user’s
loss of vision.
Consultant to attorney for the plaintiff
concerning analysis of failed hang
glider D-rings.
Mastercraft vs. Mitsubishi (1979-90506),
consultant to Condon & Forsyth for
inspection of Mitsubishi MU-276-N321MA
plane crash.
Consultant to CEC Drilling (1979-90507)
concerning analysis of failed drill
pipe.
Ranger I Collapse (1979-90510),
consultant to U.S. Coast Guard
concerning collapse of off-shore
drilling rig south of Galveston, TX.
Report to Hartford Insurance Company
(1979-90613) concerning failure of
Geosource hook assembly.
Consultant to Tooltec, Inc. (1979-90722)
concerning failure analysis of drill
pipe.
Consultant to attorney for plaintiff
(1979-90804) concerning evaluation of
steering mechanism of vehicle involved
in one-vehicle accident.
Report to GAB Business Services, Inc.
(1979-90813) concerning fracture
analysis of mechanical winch pin
failure.
Boos vs. Oklahoma Disposal (1979-90834),
consultant to attorney for defendant
concerning design and modification of a
refuse compactor.
Crosslands A & A vs. Hinkle/McCoy,
(1979-90915) consultant to insurer
concerning metallurgical analysis of
welded tow bar failure.
Report to Western Claims, Inc.
(1979-91002) concerning evaluation of
explosion and fractured gas lines from
wall heater.
Consultant to Mendes and Mount
(1979-91003).for inspection and tear
down of a Continental aircraft engine.
Report to Moran Brothers (1979-91016)
concerning examination, testing and
failure analysis of four-foot box tool
joint.
Report to Western Claims (1980-00102)
concerning investigation of welded
Link-Belt HC-138 65-ton truck crane
failure.
Arson investigation for INA (1980-00108)
and consultant to attorney for
defendant.
Report to 3-Spirits Oil & Gas concerning
investigation of swab cable failure
(1980-00302).
Consultant to State Farm Insurance
(1980-00304), concerning investigation
of chimney chase cover involved in
residential fire.
Jones vs. Otis Engineering (1980-00308),
consultant to attorney for plaintiff
concerning evaluation of down-hole
debris.
Murray vs. Huffman Mfg. (1980-00313),
consultant to attorney for plaintiff
concerning failed bicycle components.
Petersburg vs. Brown-McKee (1980-00325),
consultant to attorney for defendant
concerning grain elevator explosion
damage.
Kibby vs. Williams (1980-00402),
consultant to attorney for plaintiff
concerning evaluation of accident
involving 4-wheel drive front axle arm.
Wainoco vs. Picoma (1980-00405),
consultant to attorney for defendant
concerning investigation of failed
11-7/8" casing in gas well.
Grove Crane Collapse (1980-00410),
consultant to Western Claims concerning
structural damage to mobile truck crane.
Report to American International Group
(1980-00507) concerning failure analysis
and wreckage evaluation of collapsed
landfill truck trailer.
McBride vs. Kawasaki (1980-00512),
consultant to attorney for defendant
concerning investigation of motorcycle
fuel tank explosion.
Edwards vs. Fruehauf (1980-00515),
consultant to attorney for defendant
concerning investigation of separation
of truck trailer.
Report to CNA Insurance (1980-00516)
concerning failed welded trailer
coupling.
Horton vs. Mono Mfg. Co. (1980-00519),
consultant to attorney for plaintiff
concerning brush hog wheel rim
explosion.
Report to American Farm Bureau Service
Company (1980-00524) concerning plow
disc property evaluation.
Flatt vs. Jackson (1980-00602),
consultant to Liberty Mutual Insurance
Co. concerning failed welded truck
trailer axle.
Report to Liberty Mutual Insurance Co.
(1980-00603) concerning Freightliner
truck accident.
Brio Petroleum vs. White Mfg.
(1980-00608), consultant to attorney for
defendant of steering box & pump on 1980
Western Star tractor trailer.
Report to attorney for the plaintiff
(1980-00618) concerning investigation of
failed 8 inch water main.
Consultant to attorney for the plaintiff
(1980-00708) concerning chipping from
wedge and hammer.
Report to Western Claims (1980-00715)
concerning contribution of fractured
welded spring hanger bracket to
one-vehicle truck accident.
Haney vs. Ford Corp. (1980-00810),
consultant to attorney for plaintiff
concerning investigation of 1974 Ford
pickup truck fan blade failure.
Report to attorney for the plaintiff
(1980-00820) concerning failed seat bolt
on 1974 BMW automobile.
Northrup vs. Robert Shaw (1980-00821),
consultant to attorney for plaintiff
concerning controller failure and
propane water heater explosion.
State of Arkansas vs. Fuller
(1980-00901), consultant to attorney for
defendant of truck/automobile accident
involving separation of welded truck
axle.
Consultant to attorney for the plaintiff
(1980-00908), evaluation of captain's
seat/chair separation from a Chris Craft
Excalibur yacht.
Report to Great Southern Production Co.
(1980-00909) concerning evaluation of
failed 9/16 inch wire rope swab line.
Report to Hartford Insurance Group
(1980-01001) concerning explosion during
inflation of an aluminum automobile tire
rim.
Report to the plaintiff as to the cause
of a tire-rim separation during
inflation (1980-01007).
Report to Western Claims, Inc.
(1980-01017) concerning investigation of
one-vehicle truck accident involving
rollover of drilling rig.
Report to GAB Business Services, Inc.,
(1980-01019) concerning examination of a
trailer hitch pin.
Oliver vs. Superior Concrete
(1980-01026), consultant to attorney for
defendant concerning possible failure of
a concrete panel tilt-up insert.
Report to attorney for the plaintiff
(1980-01105) in the evaluation of a
2-3/8 inch, 4.7# J-55 tubing failure and
resulting explosion.
Snowden vs. Atchison, Topeka & Santa Fe
Railroad (1980-01112), consultant to
attorney for plaintiff concerning
failure of locomotive seat/chair.
Cox vs. Lee Way (1980-01113), consultant
to defendant concerning evaluation of
failed truck spring hanger bracket
components.
Analysis and report to Moran Energy
(1980-01114) concerning failed 5-inch
grade E drill pipe.
Investigation for INA (1980-01115) on
collapse of Christian International Rig
No. 24.
Research for Mapco, Inc. (1980-01203)
concerning design and materials for
hydrofluoric acid pressure vessel.
Analysis for EFDYN, a division of
Autoquip Corp., Guthrie, Oklahoma
(1980-01212), of case depth and chrome
plating thickness.
Research and report to Marathon Battery
Co., Waco, Texas (1980-01212) concerning
nickel/cadmium battery plate
embrittlement.
Consultant to attorney for the defendant
(1981-10101) concerning chain failure
and scaffolding collapse.
Mastercraft vs. Mitsubishi Aircraft
International (1981-10103), consultant
to attorney for defense for the crash of
Mitsubishi MU-2 aircraft.
Report to An-Son Corporation
(1981-10106) concerning a Hydril fitting
failure.
Dan Smith vs. Travel Equipment Corp.
(1981-10109), consultant to attorney for
defense concerning a flared copper
fitting.
Research and failure analysis of
sprocket segment for CMI Corporation
(1981-10110).
Investigation for United General
Insurance Co. (1981-10123) concerning
failed traveling block hook on drilling
rig.
City & Co. of Denver vs. ITT Grinnell
Corp, Eby Construction Co. (J10124)
consultant to defendant concerning
welding defects in 108” conduit.
Report to CMI Corp. (1981-10128)
concerning sprocket and shaft material
analysis.
Dunn vs. Modrak (1981-10202), consultant
to attorney for plaintiff concerning a
failed condylar plate.
Symmonds vs. Cotton Petroleum
(1981-10203), consultant to attorney for
the defendant concerning surface casing
rupture.
John Thompson/Estate of Sharon K. vs.
Harley-Davidson (1981-10207), consultant
to attorney for defendant of a
motorcycle accident.
Research and failure analysis for
Petroleum Resources (1981-10209)
concerning a failed section of 2
3/8-inch tubing.
Consultant to VePed Traffic Controls
Corp. (1981-10210), research and
evaluation of weld processes.
Consultant to LARCO Mining &
Metallurgical Co., Athens, Greece
(1981-10217), investigation of acetylene
tank explosion.
Courtney vs. Johnson Wax and American
Can Co. (1981-10219), investigation of
aerosol can explosion.
Shelton vs. Ford Motor Co. and Southwest
Ford, Inc. (1981-10405), consultant for
attorney for defendant.
Evaluation of welding process for VePed
Traffic Controls Corporation
(1981-10415).
White Stripe Pipe Inspection
(1981-10421), failure analysis of 4-1/2
inch drill pipe.
Consultant for Anschutz Corp.
(1981-10514), investigation of failure
of 5-1/2 inch casing.
Consultant for Anschutz Corp.
(1981-10515) investigation of API
conformance check and failure analysis
of 2-7/8 inch tubing.
Investigation for defense attorney
(1981-10519), concerning failed 2-7/8”
tubing.
N.L. Acme Pipe Co. (1981-10601),
investigation of failure of drill pipe.
Gulfstream American Corp. (1981-10602),
analysis of windshield materials.
Consultant to General Motors Corp.
(1981-10603) investigation of recurring
failures in X-678 conveyor chain.
Stewart vs. Jaswell Corp. (1981-10614),
investigation for attorney for
plaintiff of welded pull down drilling
rig assembly.
Investigation and analysis of fire
damage to drilling rig substructure for
Universal Resources Corp., (1981-10701).
Hodge vs. Lockheed Aircraft
(1981-10707), investigation for attorney
for the plaintiff of control cable
failure.
Douglas Parks vs. Meither Machine Co.
(1981-10712), investigation for attorney
for defendant of compressor
components involved in natural gas
processing station explosion.
Taylor vs. Ford Motor Co. (1981-10716),
investigation for attorney for
plaintiff of Thunderbird automobile
transmission assembly.
E & M Machine Shop vs. Brown Welding
Supply (1981-10717), investigation for
attorney for the plaintiff of acetylene
tank explosion and fire.
James Pitts vs. Gold Star Drilling
(1981-10725), investigation for attorney
for the plaintiff of mast failure on
drilling rig.
Plow disc physical property
determination for American Farm Bureau
Services (1981-10726).
Pride Oilfield Services, Inc.
(1981-10729), investigation and report
concerning the collapse of drilling rig.
Shar-Lane Oil Company .(1981-10732),
analyzed failure of 4-1/2 inch grade E
drill pipe.
Pride Oilwell Services (1981-10733), NDT
inspection of drilling rig.
Wright Airlines vs. General Dynamics &
TEMPCO (1981-10804), investigation for
attorney for defendant of hydraulic
cylinder piston failure.
Mid-Continent Casualty Company
(1981-10812), evaluation of a bull plug
failure.
Moran Energy Corporation (1981-10813),
research and failure analysis of a
4-1/2" drill pipe.
Badgett Steam Lube Corporation
(1981-10817), materials evaluation.
Investigation and report to The Hartford
Insurance Group (1981-10829) concerning
multiple sucker rod failures.
Trojan vs. Buckingham (1981-10830),
investigation for attorney for
defendant of an accident involving
utility pole climbing spikes.
Cheshire Adjustments (1981-10832),
investigation for attorney for
defendant of drilling rig lifting eye
failure and rig collapse.
White Stripe Pipe Inspection
(1981-10907), investigation and analysis
of failed drill pipe.
Cheshire Adjustments Co. (1981-10915),
investigation of drilling rig collapse.
Pengo Industries (1981-10916), analysis
of drill collar failure.
Royal Insurance Company (1981-110J05),
examination and investigation of a
failed wire rope.
Gibraltar Exploration (1981-110J06),
analysis of drill collar box tool joint
failure.
Crawford and Company (1981-110J08),
evaluation of 9/16-inch wire rope
failure.
Anschutz Corporation (1981-110J10),
research and evaluation of ¾ inch sucker
rods.
Report to the attorney for the defense
(1981-J11131), concerning accident
involving a 1981 Chevrolet pickup truck.
Hunt vs. AMF (1981-J11131), consultant
to attorney for defendant of an
accident involving a Harley-Davidson
motorcycle.
Analysis of bimetallic strip failure for
Sooner Engineering (1981-J11137).
Anschutz Corporation (1981-J11138),
evaluation of wire rope failure.
Corporate Air Services, Inc. vs.
Mitsubishi Aircraft International, Inc.
(J11139), investigation for attorney for defendant of an aircraft accident.
Helmerich & Payne (1981-J11231),
analysis of 5-1/4 inch diameter keyed
shaft failure.
Dickson Industries, Inc. (1981-J11232),
chemical analysis of an abrasion
resistant cast iron.
Southwest Inspection (1981-J11233),
research and report of analysis of
failed 2-7/8 inch tubing.
Wilson vs. Bollinger (1981-J11251),
investigation for attorney for
defendant of accident involving
defective truck-trailer axle failure.
Robertson vs. Sturm (J20131), consultant
to attorney for plaintiff in the
matter of the explosion of an automatic
rifle.
Israel Aircraft Industries International
(J20132), examination of landing gear
failure.
Lee Way Motor Freight, Inc. (J20133)
report concerning analysis of failed
tractor-trailer hitch pin.
Moran Energy Corporation (J20134),
failure analysis in the matter of two
failed joints of 4-1/2 inch S-135 drill
pipes.
Western Claims (J20136), examination of
a fractured diesel engine connecting
rod.
Star-Spencer Elementary School, Spencer,
Oklahoma (J20137), consultant to
attorney for plaintiff of a boiler
explosion at the school.
Research and report for The Hartford
Insurance Co. (J20138) concerning
rupture of a 24-inch oil transportation
line near Des Moines, Iowa.
Challenger Drilling vs. Cudd Pressure
Control (J20234), investigation for
attorney for defendant of an oil
well explosion.
Cactus Feeders & Ranger Ins. vs. WEMCON
Corp. (J20235), investigation for
attorney for defendant of explosion and
fire in a cattle feedlot.
U.S. Environmental Protection Agency
(J20236), investigation of drums leaking
hazardous materials Testimony before
Grand Jury in Houston, Texas.
Research and failure analysis for Moran
Brothers Energy (J20238), concerning a
failed 5-inch Grade E drill pipe from
Drilling, LTD. Rig 39.
Barber vs. Dutro (J20351), investigation
for The Hartford Insurance Group in the
matter of collapse of a four-wheel
moving cart.
Gram vs. Eastern Mountain (J20352),
consultant to attorney for defense
concerning explosion of a Primus torch
canister.
Karr vs. Synthes (J20434), consultant to attorney for plaintiff of a faulty
metal plate placed in plaintiff's right
thigh resulting in nerve damage.
Parker vs. Synthes (J20435), consultant
to attorney for plaintiff in the
matter of personal injury caused by a
faulty metal plate.
Research and report for Associated
Aviation Underwriters (J20436), of a
Bell 222 helicopter crash near Hinton,
Oklahoma.
W & B Drilling vs. Cardinal Pipe &
Equipment (J20532), consultant to
attorney for defendant of tool joint
failures.
Frank Yancy vs. Big Three Industries
(J20632), consultant to defendant
concerning cause of an acetylene tank
rupture and subsequent fire.
Schick Oil & Gas (J20639), consultant to
plaintiff for identification of 1200
feet of 2-7/8" tubing and type of
corrosion.
Furrs vs. Interlake Crane (J20652),
consultant to attorney for plaintiff
concerning evaluation of a bronze gear
failure.
Troyet Ray vs. Anderson Clayton Co. &
General Electric Co. (J20730),
consultant to attorney for defendant of
electrical fuse/switch box explosion.
Black vs. Furrs (J20732), consultant to
attorney for defendant concerning
collision between tractor-trailer and
stalled passenger vehicle.
Brantley Helicopter Crash (J20737),
consultant to attorney for defendant
concerning possible failure of
helicopter tail rotor.
Mozingo vs. Fafnir (J20830), consultant
to attorney for defendant of bearing
failure and crash of agricultural spray
airplane.
Bible vs. Buckeye Gas Products (J20831),
consultant to attorney for defendant for
failure of control valve and propane
explosion.
LeMay vs. General Motors (J20838),
consultant to attorney for defendant
concerning evaluation of a vehicle
rollover and axle failure.
Report to Howard Thornhill, Midstates
Analytical Laboratories (J20930) of
Incone l sheath corrosion.
Dan Miller vs. Sheplers, Inc. (J20839),
consultant to attorney for defendant
concerning failure of trailer tie quick
release snap.
Report (J20932) to The Hartford
Insurance Company, Denver, Colorado,
concerning operation of a side boom
crawler tractor.
Ratzlaff vs. Beltran & Welltech, Inc.
(J20934), consultant to attorney for
defendant concerning investigation of
portable drilling rig wheel failure.
Parker vs. Orion (J20936), consultant to
attorney for defendant of radio antenna
and mounting pole for evidence of
electrical contact and arcing.
McDonough Brothers, Inc., vs. Braniff,
International (J20937), consultant to
attorney for plaintiff of locking device
on maintenance stand.
Report (J21031) to Bill Page, U.S.
Companies, Dallas, Texas, metallurgical
examination of right main landing gear
from 1979 Citation I airplane.
Loyds vs. U.S. Steel (J21032),
consultant to attorney for defendant of
tubing and casing failure in
relationship to a gas well explosion.
Wayne Paiz vs. Bernard Lucero (J21034),
report for National American Insurance
Co. for evaluation of trampoline spring
failure.
Lonnie Northcliff vs. Bennett & Harris
Propane (J21035), consultant to attorney
for defendant of failure of gas fitting
and fire.
Rambler Oil Co. vs. Shiloh Drilling
(J21130), report to plaintiff concerning
failure of 8-5/8 inch casing.
S.E. Exploration vs. Brock Hydrocarbon
(J21131), third party arbitration report
to plaintiff and defendant of failed
casing.
Estella Tuck vs. Dalworth Tank, Inc.,
(J21134), consultant to attorney for
defendant of tanker truck rollover and
explosion.
Donald Stam vs. Hutchison Division of
Royal Ind. & Dutton Lainson Co.,
(J21135), consultant to attorney for
defendant of collapse of grain auger.
Report (J21136) to Nolan Systems, Inc.
concerning 5/8-inch diameter hardened
shaft failure.
Tippitts vs. Nissei (J21137), consultant
to attorney for plaintiff concerning
evaluation of thread damage inside a
drilled hole.
Report to Eby Construction Co., Wichita,
Kansas (J21138) concerning evaluation of
welding failure in 108-inch diameter
water pipe.
Jerry Cochran & David Coffman vs. Robert
Guilliemo, Martinex & MCG Picture Frames
vs. Sears and Ford Motor Co. (J21230),
consultant to attorney for defendant
concerning a failed brake line.
Hurtado vs. RodRic Corp. (J21232), N. TX
Exploration vs. Fort Worth Supply
(J30130), consultant to attorney for
plaintiff for a casing failure.
Report to The Hartford Insurance Company
(J21240), concerning a boom failure on a
concrete pumper truck.
S&T Drilling vs. J-Co Machine Works
(J21243), consultant to attorney for
plaintiff concerning an improperly
prepared wire rope socket failure.
North Texas Exploration vs. Fort Worth
Supply (J30132), consultant to attorney
for plaintiff for evaluation of a casing
failure.
Report to Dr. Richard Moore Consultants
(J30132) concerning an evaluation of
Ellis County bridge collapse.
Johnson vs. Musslewhite Trucking & Rig
Building & Worley's Welding Works
(J30134), consultant to attorney for
defendant for weld failure.
Erway vs. MacWhyte Rope Co. (J30135),
consultant to attorney for defendant
concerning failure of wire rope used in
sea water application.
Barber vs. Cessna, AAR, Inc., Bird, OKC
Flight & Airman & OG&E (J30137),
investigation for attorney for defendant
of aircraft engine components.
Harrison vs. Odell Gelvin & Steve
Wilmoth d/b/a G&W Farms (J30138),
consultant to attorney for plaintiff of
flying fragment causing eye damage.
Timothy Robertson vs. Valmont Industries
(J30139), consultant to attorney for
defendant concerning the evaluation of a
crank handle failure.
Report to insurer of F. W. Drilling
(J30232) of the failure of a wellhead
which cracked at the point where surface
casing entered the wellhead.
Briscoe Oil vs. NL Industries (J30234),
consultant to attorney for defendant
concerning failure of a down-hole tool.
Benson vs. Bell Textron (J30311),
consultant to attorney for plaintiff
for evaluation of spherical bearing
failure.
Mildred Simmons vs. OKC Airport Trust
Authority & Herman Miller, Inc.
(J30329), consultant to attorney for
plaintiff of chair bracket failure.
Consultant to Moran Energy Corp.
(J30335) analysis of failed 6-1/4 inch
OD drill collar cracked in elevator
recess area.
Consultant to Mitsubishi attorney for defendant (J30336), concerning
evaluation of in-flight breakup of MU-2
during snow storm.
King vs. Arkla (J30401), consultant to
attorney for plaintiff' of explosion
as a result of gas leakage from a gas
transmission system.
C's Mobile Home vs. Gehring Ind. &
Riblet Mfg. (J30501), consultant to
attorney for plaintiff for fracture of
welded mobile home frame.
Bender vs. Swineys (J30507), consultant
to defendant concerning pulley failure
which allowed a work table to drop.
Richard Hall vs. Ashland Oil Company
(J30516), consultant to attorney for
defendant, about failure of pipeline
used to transmit chlorine gas.
Consultant to insurer of Brentwood
Forrest Apartments (J30517) concerning
flexible gas line failure and its
relationship to apartment fire.
James Lickenbrock d/b/a All Steel Mfg.
Co. (J30522), consultant to attorney for
defendant concerning trailer lug bolt
failure which damaged classic antique
car.
Consultant for Grace Petroleum (JP30614)
concerning evaluation of failed 1-1/4
inch OD drill pipe.
Investigation of 1978 Freightliner lug
bolt failure (JP30646), for insurance
carrier.
Consultant to the State of Idaho
Department of Transportation (J30716),
evaluation of remanufactured A-588
bridge I-beams.
Consultant to Owner's insurer (J30813)
concerning fire damage evaluation on a
gooseneck trailer.
Denny vs. City of Pryor Creek Municipal
Utility Dept. (J30820), consultant to
attorney for defendant of metal joint in
gas explosion.
Moran Energy Corp. (J30833), consultant
concerning evaluation of H2S damage to
drilling rig #68.
Pride Oil Well Service Co. (J30834),
consultant concerning the evaluation of
a Pride Oil Well Service rig hydraulic
cylinder failure.
Hurst Pipe Sale, Inc. (J30835)
consultant concerning API conformance of
8-5/8 inch K-grade casing.
Consultant to U.S. Dept. of
Transportation, Nattional Transportation
Safety Board (J30843), concerning
breakup of S.S. MARINE ELECTRIC.
Texaco vs. Cudd High Pressure (J30909),
consultant to attorney for defendant,
concerning the evaluation of explosion
of a blowout preventer.
Consultant to insurer of rig owner
(J30919) concerning the evaluation of a
wire line failure in Gillette, Wyoming.
Saner & Staffs vs. Dressers Industries,
Bankhead, Inc., Aztec Specialty Co., &
Zip Tool (J30950), consultant to
attorneys for plaintiff concerning
welding defect and its influence on rig
collapse.
Consultant to attorney for defendant
(J30952) concerning the evaluation of a
flexible gas line failure and its
relationship to fire causation.
American Enterprises vs. White Motor &
General Motors Corp. (J31001),
consultant to attorney for plaintiff of
fire damage to a garbage truck starter
solenoid.
Consultant to attorney for defendant
(J31004) concerning an evaluation of a
hole in a truck brake hydraulic line.
Consultant to attorney for the Lubbock
City/County Health Department (J31024)
concerning a water heater/boiler
explosion.
Consultant to attorney for defendant,
Fairchild Industries, Inc. (J31038),
concerning in-flight fire on Air Canada
DC-9 airplane crash.
Consultant to attorney for plaintiff
(J31042), concerning left rear wheel
loss from 1983 F-350 Crew 4-Door truck
and horse trailer.
Welbros Drilling Co. vs. Seville-Grident
Corp. (J31102), consultant to attorney
for plaintiff concerning failure of
X-Hole 6 inch drill collar.
Consultant to committee for
plaintiff (J31113) concerning
metallurgical evidence involved in I-95
Mianus River Bridge collapse.
Report to Insurer of Leon Hixon, Okie
Foundation & Drilling Co. (J31148)
concerning failure effect on foundation
drilling truck stability.
Consultant to Fair Oil Co. (J31216)
concerning 2-3/8 inch collapsed tubing
from HS Davenport #1 well.
Consultant to Suit's Drilling Co.
(J31237) concerning failure of steel
cast pulsation dampeners.
Sharp vs. Dayton Hudson & Huffy Corp.
(J31238), consultant to attorney for
plaintiff concerning handlebar failure
on motor-cross bicycle.
Kirksey vs. D.C. Well Service & Texaco,
Inc. (J40116), consultant to attorney
for defendant concerning failures of
anchor I-bolts and turn-over of
work-over well service unit.
Santa Fe vs. Butler Mfg. and Ohalaran
Oil (J40158), consultant to attorney for defendant concerning tank explosion.
Kay vs. Quick Sharp Inc. (J40321),
consultant to attorney for plaintiff
concerning failure of a ceramic knife
sharpener.
Consultant to truck owner (J40340)
concerning the evaluation of steering
column bracket failure and its relation
to an accident.
Consultant to insurer of coal company
scraper (J40410) concerning the
evaluation of fire damage to a
scraper/tractor frame.
Consultant to insurer (J40465) of quick
print film processor concerning the
failure, design, and manufacture of
water filter casing.
Brackett vs. Ryder Truck Rental, Inc.
(J40529), consultant to attorney for
defendant concerning disengagement of a
wheel from a tractor trailer.
Vosler vs. Leede Oil (J40543),
consultant to attorney for defendant
concerning failure of a chicksan line.
Pride Oil Well Service vs. Cooper Mfg.
(J40616), consultant to attorney for
plaintiff concerning defects in
structural members of well servicing
rigs.
Oxley Petroleum vs. Voest-Alpine
(J40629), consultant to attorney for
plaintiff concerning defects in drill
pipe.
Kincade vs. Brown Tool and Supply
(J40633), consultant to attorney for
defendant concerning a fatigue failure
of a drill collar.
Oklahoma City Municipal Authority vs.
GHA Lock Joint (J40659), consultant for
plaintiff of failure of spiral wire
reinforced concrete water conduit.
Consultant to insurer (J40908) of Walls
Bargain Center roof collapse in Midwest
City, Oklahoma.
Hutchinson vs. Rockwell International
(J41025), consultant to attorney for
plaintiff concerning a flying fragment
from a truck axle.
Consultant to insurer of owner of
aircraft (J41035) concerning failure of
an aircraft engine crankshaft.
Carter vs. Harnischfiger (J41073),
consultant to attorney for defendant
concerning failure of attachment bolts
in an overhead crane.
Kennecott Metals vs. Teton Exploration
&Drilling (J41127), consultant to
attorney for defendant of welding
defects in large hole mine shaft.
Consultant to attorney for plaintiff
(J41212) concerning evaluation of a wire
rope failure.
Tenneco vs. Patterson (J41216),
consultant to attorney for defendant
concerning evaluation of a fatigue
failure in offshore drilling string.
Kerr Glass Co. vs. Big Three (J7D1007),
investigation of failure of acetylene
generator gasket resulting in release of
acetylene and subsequent explosion.
Oklahoma Tank Trucks vs. Walter Conner
(JAC060), consultant to attorney for
defendant concerning an explosion of a
hot oil unit.
Wallace vs. Briggs & Stratton (JAC200),
consultant to attorney for defendant
concerning failure of an aluminum
flywheel housing.
Consultant to attorney for the defendant
Nineteenth Seed (JAD090) concerning
failure of a dump truck leaf spring.
Higgins vs. Woodings-Verona Tool Works
(JAD120), consultant to attorney for
defendant concerning chip flying from
striking tool.
Cash vs. Litton Ind. (JAD140),
consultant to attorney for plaintiff
concerning a chip flying from a hammer.
Moffat vs. Kelsey Hays (JAD250),
consultant to attorney for defendant
concerning failure of wheel studs.
Consultant to oil company (JAD420)
concerning failure of 3-1/2 inch, 15.8#
internally coated tubing.
Consultant to attorney for defendant
(JAD540) concerning failure of a power
sander.
Consultant to oil company (JAD570)
concerning circumferential cracking in
P-100, 38# casing.
Tulak vs. Brockway Glass (JAE040),
consultant to attorney for defendant
concerning failure of a glass container.
Consultant to aircraft manufacturer
(JAE180) concerning failure of landing
gear outer body.
Xerox vs. J.A. Jones Construction Co.
(JAE330), consultant to attorney for
plaintiff concerning faulty installation
of a PVC piping system.
Consultant to Eby Construction, Wichita,
Kansas (JAG090) concerning alleged
defective welding in a water pipeline.
Washut vs. Cudd Pressure (JAG190),
consultant to attorney for defendant
concerning a well explosion.
Union Oil vs. Patterson (JAG240),
consultant to attorney for defendant
concerning failure of a pup joint.
Green vs. Sears & Fisher Heating
(JAG530), consultant to attorney for
defendant concerning an alleged faulty
furnace installation.
Consultant to Overton Construction
(JAH090) concerning evaluation of I-beam
discontinuities.
Ford vs. Cabot Corp. (JAH130),
consultant to attorney for defendant
concerning failure of a casing head.
Prufrock Ltd. vs. USAIG (JAH270),
consultant to attorney for plaintiff
concerning premature failure of an
aircraft engine.
Clements vs. Lockwood Corp. (JAI440),
consultant to attorney for plaintiff
concerning an electrocution from an
irrigation system.
Consultant to the insurer (JAJ020)
concerning the explosion of Rollingwood
Elementary School.
Heald vs. M&R Industrial Coatings
(JAJ080), consultant to attorney for
defendant concerning failure of a wire
rope.
Bates vs. Ridge Tool Co. (JAJ150),
consultant to attorney for plaintiff
concerning design of a pipe threading
device.
Wampler vs. Radiator Specialty Co.
(JAJ540), consultant to attorney for
defendant concerning design and material
in automobile radiator.
Consultant to oil company (JAK100)
concerning failure of 7-5/8, 33.7#,
P-110 casing failure.
Explosion Damage at Calvary Tabernacle
Church of God, Checotah, OK (JAK230),
investigation of building damage
resulting from bomb explosion on nearby
highway (I-40).
Smith vs. General Electric (JAK250),
consultant to attorney for defendant
concerning arcing in a fuse box
explosion in plaintiff’s face.
Consultant to insurer (JAK370)
concerning the failure of a gate valve
in the Wilson Public School.
Consultant to manufacturer (JAL480)
concerning failure of a tail pin in an
oil well pump.
Mathews vs. Cudd Pressure (JBA020),
consultant to attorney for defendant
concerning failure of an oil well
lubricator.
Consultant to oil company (JBA100)
concerning cracking of a drill collar.
Ferguson vs. Padre Tubular Inc.
(JBA180), consultant to attorney for
defendant concerning failure of oil well
tubular goods.
Freezer Service vs. U.S. Supply
(JBA580), consultant to attorney for
defendant concerning an explosion in an
ammonia freezer plant.
Ruiz vs. Rochester Corp. (JBA590),
consultant to attorney for defendant
concerning failure of a wire rope.
Sledge Welding vs. General Processing
(JBA600), consultant to attorney for
defendant concerning an acetylene
cylinder fire.
Potlatch Corp. vs. Sirrine Services
(JBA610), consultant to attorney for
defendant concerning an explosion in a
black liquor plant.
Consultant to insurer of child care
facility (JBB100) concerning evaluation
of a toy failure.
Landrum vs. Acadian (JBB110), consultant
to attorney for plaintiff concerning
failure of a flexible gas line.
Keith vs. General Motors (JBB150),
consultant to attorney for plaintiff
concerning an automobile axle failure.
Robinchax vs. Georgia Boy Mfg. (JBB200),
consultant to attorney for defendant
concerning explosion of a truck fuel
tank support strap.
Sunbelt vs. Blue Quail Oil & Gas
(JBB230), consultant to attorney for
defendant concerning failure of a
blowout preventer.
Bludgett vs. APAC Caroline Inc.
(JBB340), consultant to attorney for
plaintiff concerning failure of an
automobile axle.
Lester Carolyn vs. Sears Roebuck & Co.
(JBB410), consultant to attorney for
plaintiff concerning manufacturing
defect in kerosene heater.
Consultant to manufacturer (JBB570)
concerning quality of welds produced in
presence of magnetic field.
Spiel Gut Toy Evaluation (JBC070),
investigation of toy which severed the
tip of child’s finger.
Day vs. OG&E & McCoy Tree Surgery
(JBC280 ), consultant to attorney for
defendant concerning a tree limb which
fell on electrical line igniting wooden
pole.
Ruiz vs. City of Anaheim (JBD140),
consultant to attorney for defendant
concerning failure of a window washer's
support line.
Whitley vs. Kansas City Southern
(JBD170), consultant to attorney for
defendant concerning alleged asbestos
containing firebrick.
Blood vs. Treanor (JBE090), consultant
to attorney for defendant concerning
failure of a safety screen.
Consultant to owner (JBE150) concerning
failure of a truck steering gear.
Black vs. Cabot Petroleum (JBE300),
consultant to attorney for defendant
concerning failure of an oil well
casing.
Consultant to Texaco Oil & Gas (JBE310)
concerning failure of a hammer union at
Will Rogers Airport.
Royal Swedish Tanning Salon Wiring Exam
(JBF150), investigation of building
wiring and tanning beds for fault.
State Farm Insurance vs. Fleetwood Motor
Homes (JBF200), consultant to attorney
for plaintiff concerning failure of
a flexible gas line.
James Wainwright vs. Royal Ins. Co. of
Am. (JBF210), consultant to attorney for
plaintiff in the investigation of a
relief valve.
MCI vs. Crockett Oil Co. (JBF410),
consultant to attorney for defendant
concerning alleged contamination of
motor oil.
McGiel vs. Skyhook Inc. (JBG200),
consultant to attorney for defendant
concerning failure of a cherry picker
lifting device.
Hatto vs. NW Central Pipeline (JBG370),
consultant to attorney for defendant
concerning front end loader penetration
of high pressure gas transmission line
and resulting explosion/fire.
ATV Stability Evaluation (JBG380),
consultant to attorney for plaintiff in
the evaluation of a Honda ATV rollover.
City of Mont Belvieu vs. Tenneco, et al
(JBG430), consultant to attorney for
plaintiff for failure of casing in LPG
salt dome storage system.
Kittrell vs. Aerospacial Helicopter Inc.
(JBH120), consultant to attorney for
plaintiff concerning failure of a
helicopter transmission.
Consultant to aircraft manufacturer
(JBH220) concerning the evaluation of an
AQM forward tank dome failure.
Frigon vs. Cessna (JBH300), consultant
to attorney for plaintiff of a
crankshaft failure.
Johnson vs. U-Haul (JBI190), consultant
to attorney for defendant concerning
failure of a truck brake line.
Examination of Damage to Top of Water
Tower (JBI280), investigation of
lightening and arcing damage to water
tower.
Terry Tippett vs. CMI and John Armstrong
(JBI330), investigation of the failure
of a pressure relief valve which pumps
hot liquid asphalt.
Vandall vs. Prine Petrol Products
(JBI400), investigation of a truck fuel
tank explosion.
Consultant to attorney for plaintiff
(JBJ040) concerning investigation of
Cessna 421-66PC aircraft landing gear
failure.
Wienecke vs. Synthes (JBJ060),
consultant to attorney for plaintiff
concerning failure of a femur nail.
Consultant to insurer of owner (JBJ110)
concerning a weld failure in a hot oil
pumper unit and subsequent fire and
explosion.
Morrison vs. Overhead Door (JBK170),
consultant to attorney for defendant of
overhead door which fell resulting in a
fatality.
Fierro vs. Caterpillar Tractor (JBL060),
investigation of engine failure of
Caterpillar tractor.
Tate vs. Auto Convoy (JBL300),
consultant to attorney for defendant
concerning accident involving auto
transport carrier.
Moundsview vs. Williams Pipeline
(JCB400), consultant to attorney for
defendant of a pipe rupture and
investigation of corrosion and/or
manufacturing problems.
Consultant to insurer of contractor
(JCB470) concerning collapse of the
Moore Community Center roof.
Cable Hoists of Dam Gates (JCC200),
investigation of uneven stressing of
cables used for lifting dam gates.
Reeves vs. Charles Bryant Jr. d/b/a
Charles Electric, Nutri Envelopes Inc.
and Shultz Cattle Co., Inc. (JCC230),
consultant to attorney for defendant in
the investigation of grain auger
accident.
Estate of Spicer vs. Nu-way Mobile
Homes, Virgin Lumber Co. & Rheem Mfg.
(JCC270), consultant to attorney for
defendant in the investigation of a
water heater which caused mobile home
fire.
Cooper Manufacturing vs. B & W and U.S.
Steel (JCD200), consultant to attorney
for plaintiff of defective steel
structural in oil well servicing rigs.
Consultant to insurer of owner (JCD330)
concerning failure of a Bronco
automobile axle.
Kerr McGee Waste Containers (JCD390),
investigation to evaluate material
substitution for nuclear waste
containment vessels.
Tice vs. Oakes Mfg. co. (JCE010),
consultant to attorney for plaintiff
concerning failure of a wooden
stepladder.
Consultant to aircraft manufacturer
(JCE210) concerning repeated failures of
landing gear.
Cooper vs. General Motors (JCE220),
consultant to attorney for plaintiff
concerning the sharpness of an
automotive stamping.
General Can vs. United ElChem (JCF200),
consultant to attorney for defendant
concerning failure of a series of cans.
Harmon vs. Container Products (JCG070),
consultant to attorney for defendant
for failure of a stainless steel drum
containing nitric acid.
Stephens vs. Ralston Purina (JCG160),
consultant to attorney for plaintiff
concerning a failure of pulley system in
grain elevator.
Harrison vs. Hi-Lift Equipment Rental
(JCG380), consultant to attorney for
defendant concerning failure of welded
scaffolding.
Consultant to insurer of transport
company (JCH040) concerning failure of
truck wheel studs.
Cross vs. Grace Drilling (JCH160),
consultant to attorney for defendant
concerning failure of a chicksan line.
Cudd Pressure Control vs. Thibodeaux
(JCI300), consultant to attorney for
plaintiff concerning failure of a
threaded elbow.
Wendt vs. The Coleman Co. (JCK160),
consultant to attorney for defendant
concerning explosion involving a propane
camping stove.
Trunkline LNG vs. Trane Co. (JCL110),
consultant to attorney for plaintiff
concerning alleged investigation of
stainless steel tubing.
Mesche vs. Duane's Flying Service
(JDA170), consultant to attorney for
defendant concerning failure of an
aircraft engine cylinder.
Neilson vs. Blue Diamond (JDA280),
consultant to attorney for defendant
concerning collapse of a flatbed tractor
trailer jack.
Keeton vs. Continental Teledyne
(01F80051), consultant to attorney for plaintiff concerning failure of an
aircraft engine crankshaft.
ANR Pipeline vs. Okemah Construction
(JDA410), consultant to insurer of
defendant on physical damage to a
pipeline.
Hudson vs. Albert's Plating (JDB804),
consultant to attorney for defendant
concerning an alleged defect during
plating of chair hardware.
Halliburton vs. Texas Steel (JDC805),
consultant to attorney for plaintiff
concerning casting defects.
Thanh vs. Tuthill (JDC806), consultant
to attorney for defendant concerning
failure of a high pressure fitting.
Wommack vs. Batesville Casket (JDD807),
consultant to attorney for defendant
concerning separation of a trailer from
a tractor trailer.
Diamond vs. Mitsubishi Aircraft
International (JDE808), consultant to
attorney for defendant concerning
abusive utilization of a jet aircraft.
Evaluation of a slow speed shaft failure
(JDE809) for the manufacturer of oil
well pumps.
Liftrick vs. Otis Courtwright (JDE811),
consultant to attorney for defendant
concerning the failure of a flexible gas
line.
Richardson vs. Ingram (JDE812),
consultant to attorney for defendant
concerning failure of a wire rope.
Bennett vs. City of Stillwater (JDE814),
consultant to attorney for defendant
for evaluation of an emergency flasher
light bulb filament.
N.L. Industries vs. Cimarron Exploration
(JDE815), consultant to attorney for
plaintiff concerning failure of a
fishing tool.
Cannon vs. Southern Supply (JDG818),
consultant to attorney for defendant
concerning explosion of an air tank.
Consultant to Lincoln Petroleum Co.
(JDG819) concerning casing failure.
Adams vs. Big Three Industries (JDH820),
consultant to attorney for defendant
concerning failure of an oxygen cylinder
valve.
Consultant to U.S. Army Corp. of
Engineers (88I22I) concerning failure
and testing of welded stainless steel
pipeline.
Report (JDK823) to Exxon Corp.
concerning explosion and fire in
tertiary oil recovery operation.
Ward vs. U.S. Forgecraft (JDL827),
consultant to attorney for defendant
concerning engagement of a lanyard
safety hook.
Hales vs. Chromcraft (JDL828),
consultant to attorney for defendant
concerning failure of an office chair.
Heinsch vs. Whipples and Eaton Corp.
(JDL829), consultant to attorney for
defendant for failure of a switch in a
hot tub heater system.
Report (JDL831) to Bud Hale & Co.
concerning a tire/rim failure on a
Budget car leasing company automobile.
Neil vs. Teledyne (JEA010), consultant
to attorney for defendant concerning
failure of bolts on a large capstan.
Thompson vs. Federal Pacific Electric
(JEA020), consultant to attorney for
defendant concerning failure of
electrical switch and fire.
Cornett vs. Hertz-Penske Truck Leasing
(JEA030), consultant to attorney for
defendant concerning re-welding of a
truck step bracket.
Big Three vs. Kruger (JEA040),
consultant to attorney for plaintiff
concerning a fire in an oxygen
compressor.
Stogsdill vs. Suzuki and Reynolds
(JEA050), consultant to attorney for
plaintiff concerning failure of a bolt
in a four wheel ATV.
Chapman vs. Sears (JEA060), consultant
to attorney for plaintiff concerning
failure of a chair.
Prochnow vs. Bell Helicopter (JEA070),
consultant to attorney for plaintiff
concerning failure of a tail structure
member.
Foust vs. Keller and Ace Hardware
(JED120), consultant to attorney for
plaintiff concerning failure of an
aluminum extension ladder.
55 Well Service vs. Halliburton
(JED130), consultant to attorney for
plaintiff concerning collapse of a
welded work over rig.
White vs. Makita (JEE140), consultant to
attorney for plaintiff concerning
failure of a table saw.
Investigation and report (JEE150) for
attorney for plaintiff concerning
failure of a van A-frame member.
Investigation (JEF160) for attorney for plaintiff concerning failure of a
hip joint.
Hebert/Billoit vs. Chevron and U.S.
Cylinder (JEF170), consultant to
attorney defendant concerning
explosion of an acetylene cylinder.
Morrow vs. Walker (JEF180), report to
representative of plaintiff concerning
failure of a pneumatic floor jack.
Ca-Tex vs. U.S. Steel (JEG190),
consultant to attorney for defendant
concerning failure of 3 1/2 inch X-95
drill pipe.
Hammons vs. Lemco (JEH200), consultant
to attorney for defendant concerning
failure of a telephone line stringing
tool.
Dear and Smith vs. Coyne Cylinder
(JEI220), consultant to attorney for
plaintiff concerning explosion of an
acetylene cylinder.
Investigation and report (JEI230) to the
insurer of a well servicing rig
concerning a wire rope failure.
Investigation and report (JEI240) to
attorney for insurer concerning the
failure of a water pump casing.
Davee vs. Frontier (JEI250), consultant
to attorney for plaintiff concerning
failure of a welded crane boom.
Crozier vs. Hedgecock (JEJ290),
consultant to attorney for plaintiff
concerning failure of aluminum ladder.
DeWare vs. International Harvester
(JEJ300), consultant to attorney for
plaintiff concerning a truck steering
failure.
Cameron Iron Works vs. Quality Oilfield
Products (JEJ310), consultant to
attorney for defendant concerning
alleged patent infringement.
Investigation and report (JEK320) to
Kerr McGee Corporation concerning
failure of tank car valve in
loading/unloading accident.
Bruner vs. Kearney (JEK330), consultant
to attorney for plaintiff concerning
failure of high voltage
electrical/mechanical connector.
Investigation and report (JEK340) to
Northbrook Insurance Company concerning
failure of water pump impeller pulley.
Gary vs. McKesson (JEK350), consultant
to attorney for defendant concerning
failure of a medical walker.
Investigation and report (JEK360) to
attorney for defendant K.O. Steel
Casting concerning a hammer union
failure.
Argello vs. Richard Walker Medical
(JEL370), consultant to attorney for
defendant concerning failure of a
pituitary rongeur.
Investigation and report (JEL380) to
Instrument Specialties Company
concerning an evaluation of instrument
springs.
Frances Dean vs. Big Three (JFA020),
consultant to attorney for defendant
concerning breathing of compressed
helium.
Investigation (JFA030) to attorney for plaintiff concerning the failure of
a welded boat trailer tongue.
Touchette vs. Chevron & Tricel
Environmental (JFA040), consultant to
attorney for defendant.
Archer Daniels vs. TGS Construction
(JFA050), consultant to attorney for
defendant concerning collapse of a grain
storage facility.
Jedele vs. Chrysler (JFB060), consultant
to attorney for plaintiff concerning
failure of a seat back tilt mechanism.
Santos vs. Schwing (JFB070), consultant
to attorney for defendant about drawing
translation (German to English) weld
quality/adequacy.
Clearwater Constructors vs. Central
Texas Equipment (JFC080), consultant to
attorney for defendant concerning
weld failures.
Madison Farms Elevator vs. SBC
Construction (JFD090), consultant to
attorney for defendant concerning a
grain elevator explosion.
Kerr Glass vs. Big Three (JFD100),
consultant to attorney for defendant
concerning acetylene plant explosion.
Mitchell vs. Caterpillar (JEF110),
consultant to attorney for defendant
concerning failure of fasteners on a
bulldozer seat.
Frazier vs. Bender (JFF120), consultant
to attorney for defendant concerning
failure and design of a load bender
strapping handle.
Investigation (JFH140), consultant to
Bud Hale & Company concerning protective
devices on plastic molding machine.
VE Corp vs. Allied Millwright (JFH150),
consultant to attorney for defendant
concerning the effect of welding on a
heat treated bracket.
Stanley vs. Glad, Inc. (JFI160),
consultant to attorney for plaintiff
concerning failure of overhead welded
crane equipment.
VanArsdall vs. AJC, Inc. (JFI180),
consultant to attorney for defendant
concerning spalling from a roofer’s
hatchet.
Steven K. Martin vs. Payless
Cashways/Krause (JFJ190), consultant to
attorney for defendant concerning
collapse of an articulating ladder.
Britt vs. S.E. Air Gas (JFJ200),
consultant to attorney for defendant
concerning fire/explosion sequence and
integrity of fusible plug.
Moore vs. Quality (JFK210), consultant
to attorney for plaintiff concerning
failure of scaffold board elevating
device.
Arco vs. N.L. Shaffer (JFK220),
consultant to attorney for defendant
concerning explosion of subset valve in
loss of offshore oil rig.
Hamilton vs. Hon Industries (JFK230),
consultant to attorney for defendant
concerning failure of an office chair.
Eby Construction vs. Reddy Buffalo Pump
(JGA020), consultant to attorney for
plaintiff concerning evaluation of
deformation in a pump shaft.
Huerta vs. Huber (JGA030), consultant to
attorney for defendant concerning
failure of closure on sand blasting unit
sand pot.
Midland Water Treatment Plant (JGA040),
consultant to company concerning
corrosion from inadequate
undercoating/painting.
Jet East Inc. (JGA050), metallurgical
evaluation of failure of MU-2 aircraft
nose gear.
Cabrera vs. Clyde Construction (JGB060),
consultant to attorney for defendant
about failure of weld on construction
equipment.
Williams vs. M P & L (JGB070),
consultant to attorney for defendant for
proof of installation of nut during
construction of a radio tower.
Warner vs. Forum Bowl (JGB080),
consultant to insurer of Forum Bowl
concerning evaluation of brazing failure
in a chair leg.
Johnson vs. Lone Star Gas (JGB090),
consultant to attorney for plaintiff
concerning coupling pipe corrosion and
subsequent house explosion.
Young Drilling vs. Dana Corp. (JGB100),
consultant to attorney for defendant
concerning the collapse of a drilling
rig.
Bill's Auto Parts Loss (JGE110),
consultant to attorney for defendant
for evaluation of alleged corrosion
resulting from water damage.
Atlas Lumber vs. SPS (JGE120), testimony
for attorney for tdefendant concerning
metallurgical evidence contained in
melted copper wire.
Graham vs. COBE Labs (JGF130),
consultant to attorney for defendant
concerning failure of a peritoneal
catheter.
Fisher Controls vs. Kanebridge Corp/Bolt
& Nut (JGF140), evaluation for attorney
of defendant of fastener for hydrogen
embrittlement.
Harris vs. Wheels in Motion (JGG150),
consultant to attorney for defendant
about proper attachment of bicycle wheel
to the bicycle frame.
West Texas Miracle Ear vs. Aaron Rents
(JGG160), consultant to attorney for
defendant concerning failure of
re-welded chair.
Archer vs. Big Three/Ransom Tempil
(JGG170), consultant to attorney for
defendant concerning failure of welding
head manipulator.
Gilbreath vs. Colonial Co., BMT and Mr.
Renter (JGG180), investigation of
explosion of wallpaper steamer.
Crane/Power Line Investigation (JGG190),
report to contractor concerning evidence
of contact and electrical arcing of
crane boom with electrical on conductor.
Barnes vs. Harnischfeger (JGG200),
consultant to attorney for plaintiff
concerning failure of a jib fixture.
NCNB vs. Dexter Water Mgt/Mogul
(JGH210), consultant to attorney for
defendant concerning failure of copper
tubing in building cooling system.
Smith vs. Bradford Mowing (JGH220),
consultant to attorney for defendant
concerning failure of a roadside mower
blade.
Layne vs. Bee Line (JGH230), consultant
to attorney for defendant concerning the
design and failure of a shaft in a truck
wheel alignment head.
Payton Machine vs. Coastal Chemical Co.
(JGH240), consultant to attorney for
defendant about contamination from
blowing muriatic acid.
Hernandez vs. John Deere (JGI250),
consultant to attorney for plaintiff
concerning failure of an open-end
wrench.
Bowen vs. Larkotex & Harvey Surgical
(JGJ260), consultant to attorney for
defendant concerning failure of rubber
tips on a walker.
Bill Powell Die Chip Investigation
(JGJ270), consultant to attorney for
plaintiff concerning chipping from a
machine stamping die.
Carlton Heights Apartment
Window(JGJ280), consultant to attorney
for defendant concerning
metallurgical evidence from a break-in
and rape.
Aero Oil vs. Exploreco Energy (JGK290),
consultant to attorney for defendant
concerning alleged defects in oil well
casing.
San Migual vs. Texas Highway Dept.
(JGK300), consultant to Texas Attorney
General's office concerning an
overpass/guardrail accident.
Robert Almand vs. So. Side Auto Parts
(JGL310), consultant to attorney for
plaintiff concerning failure of high
pressure hydraulic hose.
Resource Trailer vs. Fisher (JGL320),
consultant for defendant concerning
effect of cargo on corrosion in truck
trailers.
Harper vs. Hon Industries (JHA010),
consultant to attorney for defendant
concerning failure of an office chair.
Anderson Tech. vs. Great SW Marketing
(JHA020), consultant to attorney for
defendant about failure of a concrete
pre-tensioning device.
Wheeler Energy vs. Cap Rock Pipe
(JHA030), consultant to attorney for
plaintiff concerning failure of oil well
tubing couplings.
Pearson vs. SPS (JHB040), consultant to
attorney for defendant to evaluate
arcing and electrocution upon contact of
a pole and 7400 volt electrical line.
Casebolt vs Smith (JHC050),
investigation of boat accident with
question regarding the angle of attack.
Frost vs. Caterpillar (JHC060),
consultant to attorney for defendant
concerning failure of welds in triple
high warehouse fork lift.
Telelect vs. Schwing America (JHC070),
consultant to attorney for plaintiff
concerning adequacy of weld design.
U.S. vs. Zachry Construction (JHC080),
consultant to attorney for plaintiff
concerning welding of stainless steel
piping in jet fuel facility.
Casey vs. Madison Mill Sledge (JHC090),
consultant to attorney for defendant
concerning chipping from a sledge
hammer.
Orville Cumiford vs. GM, et al (JHE100),
consultant to attorney for plaintiff
concerning failure of automobile axle.
Thomas vs. Arkansas Western Gas
(JHE120), consultant to attorney for
defendant concerning failure of a gas
line.
Henderson vs. Firestone/Bridgeton
(JHE130), consultant to attorney for
plaintiff concerning failure of truck
tire split rim.
Jackson vs. AISD & General Motors
(JHE140), consultant to attorney for
defendant concerning failure of leaf
springs on school bus and disengagement
of rear wheels and axle.
Beardsley vs. Rockwell Int. (JHF150),
consultant to attorney to plaintiff
concerning chipping from a truck axle.
Fant vs. Hobbs Equipment (JHF160),
consultant to attorney for defendant
concerning failure of welded hydraulic
cylinder on cherry picker.
Garcia vs. Austin Bridge & Rickman Screw
Anchor Co. (JHF170), consultant
regarding failure during lift at
construction site of bolts securing
crane mast to crane transporter.
Blast Door Hanger Shaft Failure
(JHG180), consultant to U.S. Army Corps
of Engineers for failure of a welded
hanger door support.
LeMoine vs. Bending Shoe Man (JHI200),
consultant to attorney for plaintiff
concerning failure of an aluminum tubing
bender.
Martinez vs. Bailey & Mayhew (JHJ210),
consultant to attorney for plaintiff
concerning chipping of a hand tool.
Galvin vs. V. Waldon, et al (JHJ220),
consultant to attorney for plaintiff
concerning rusting and failure of truck
trailer.
Dansby vs. Barret, Inc. (JHJ230),
consultant to attorney for defendant
concerning an explosion of oil storage
tank.
Patterson vs. Maintain, Inc. (JHJ240),
consultant to attorney for defendant
concerning failure of welded oilfield
truck trailer hitch.
Sandusky vs. Caterpillar (JHK250),
consultant to attorney for defendant
concerning failure of a wire rope on a
pipe layer.
Cokinos vs. L.B. Foster (JHK260),
investigation of pipeline failure.
McIntyre vs. SPS (JHK270), consultant to
attorney for defendant concerning wear
of electric wiring.
Weld Failure/Compressor Inlet (JHK280),
report to plaintiff’’s insurer
concerning failure of a jet engine
compressor inlet.
Wittenburg vs. SPS (JHL300), consultant
to attorney for defendant concerning
failure of an electrical line/wire
leading into a residence.
Stephenson/Taylor Estate vs. RHS
(JHL320), consultant to attorney for
defendant concerning failure of oil
field hydraulic pulling jack.
TCO vs. Rockwell International (JHL330),
consultant to attorney for plaintiff
concerning in-flight wing separation
from Gulfstream aircraft.
Oxley vs. Picoma Industries (JIA010),
consultant to attorney for defendant
concerning failure of oil field casing
couplings.
Ragsdale vs. S.W. Research (JIA020),
consultant to attorney for defendant
concerning failure of a welded trailer
tongue.
Enloe Aluminum Canopy Failure (JIB030),
report to defendant's insurer
concerning failure of an aluminum
canopy.
Bryant vs. Rockwell (JIC040), consultant
to attorney for plaintiff concerning
chipping from a truck axle.
Fuentes vs. Dana Corp. (JID050),
consultant to attorney for defendant
concerning collapse of a repaired
drilling rig.
Quaker Oates vs. Engineers (JID060),
consultant to attorney for defendant
concerning failure of a valve.
Olson vs. Chance (JID070), consultant to
attorney for defendant concerning
failure of wire rope on a carnival ride.
Aston vs. SPS (JID080), consultant to
attorney for defendant concerning a
range fire due to arcing from a high
voltage electric line.
Beavers vs. Sisson (JID090), consultant
to attorney for defendant concerning
failure of a gas line valve and
propane/butane explosion/fire.
Dykes vs. GESCO (JIE100), consultant to
attorney for defendant concerning
failure of an automobile generator.
Nichols & Stanley vs. Georgia Pacific
(JIF130), consultant to attorney for
plaintiff concerning corrosion and
failure of welded overhead walkway.
Highway Mower Debris (JIG150), report to
attorney for insured concerning
evidence and debris evaluation.
Big Three CO2 Rupture (JIH160) report to
owner concerning rupture of a CO2
cylinder.
Hutchison vs. Dana (JIH170), consultant
to attorney for defendant concerning
drilling rig collapse.
Mapco vs. Flint (JIH180), consultant to
attorney for defendant concerning
failure of welded ammonia pipeline.
Hercus vs. Peterson (JIH190), consultant
to attorney for defendant concerning
failure of vice grip pliers.
-- vs. American Tool (JII190),
investigation of alleged tool failure
that dropped I beam on plaintiff.
Burkett vs. Custom Accessories (JIJ200),
consultant to attorney for plaintiff
concerning failure of load binding tie
down.
Gardner vs. Goodyear (JIJ210),
consultant to attorney for plaintiff
concerning a vehicle falling from
elevated hydraulic automotive rack.
Slough vs. Eby Construction (JJJ211),
consultant to attorney for defendant
concerning arcing and electrical contact
of crane and high-voltage electrical
line.
Ellsworth Motor Freight Hopper Lid
(JIJ230), consultant to insurer of a
truck line of failure of aluminum cast
hopper lids on truck trailers.
Tulsa School Board Goal Failure
(JIJ240), consultant to attorney for
school board concerning corrosion and
adequacy of welded soccer goal.
Central & Southwest vs. Poz Lok
(JIK250), consultant to company
concerning failure of copper
tubing/fittings in a fire sprinkler
system.
Horner Food vs. AAA Refrigeration
(JIK260), consultant to attorney for
defendant concerning corrosion due to
placement of a refrigerant line.
Cline vs. King Machinery (JIK270),
consultant to attorney for defendant
concerning failure of an air driven
pneumatic wrench.
Hoyle vs. Black & Decker (JIL280),
consultant to attorney for defendant
concerning arcing and failure of a
switch in an electric hand tool/wrench.
Williamson vs. Cannondale Corp.
(JJA010), consultant to attorney for
defendant concerning a weld failure on a
mountain bicycle.
Beamer vs. Versa (JJA020), consultant to
attorney for defendant concerning
failure of articulating ladder.
Whitebead School District Chain Failure
(JJC030), consultant to insurer of
school district concerning chain failure
on school yard swing.
Beamer vs. Wiscraft (JJC040), consultant
to attorney for defendant concerning
failure of articulating ladder.
Harrison vs. Chance (JJC050), consultant
to attorney for defendant concerning
failure of come-along aluminum casting.
Oxygen Pipeline/Valve Explosion
(JJD070), investigation of explosion of
oxygen from improperly installed oxygen
valve.
U.S. Secretary of Labor vs. Murphy
Enterprises (JJD080), consultant to
plaintiff concerning a wire rope failure
on a carnival ride.
ReCon Construction Trailer Separation
(JJG090), consultant to insurer of
trailer vehicle involved in welded
trailer separation.
Arnold vs. Paccar/Kenworth (JJG100),
consultant to attorney for plaintiff
concerning truck muffler shield.
Cook vs. Lindberg Heat Treating
(JJG110), consultant to attorney for
defendant concerning heat treatment of a
tree spike.
Lopez vs. Gates (JJH120), consultant to
attorney for plaintiff concerning
failure of braided hydraulic hose.
Shelton & Henderson vs. Texas Utilities
Electric Co., Inc. & Texas Utility Co.
(JJI140), investigation for attorney for
defendant of arcing and electrocution
resulting from aluminum irrigation pipe
contacting overhead electrical
high-voltage line.
Vieregge vs. Lone Star Steel (JJI150),
consultant to defendant concerning
corrosion of gas pipeline and subsequent
explosion.
Parnell Dodge Caravan Rollover (JJJ160),
consultant to attorney for plaintiff
concerning rollover of Dodge Caravan and
axle failure.
Max Chisolm vs. Marshall Logging, Inc.
(JJJ170), investigation for attorney for
defendant of diesel fuel tank explosion
from welding on fuel tank.
Moore vs. Conoco (JJJ180), consultant to
attorney for defendant concerning
failure of a gasoline pipeline.
Delacerda vs. McKissic-Crosby Group,
Inc. (JJJ190), investigation for
attorney for plaintiff of door on oil
field drilling rig casting failure which
resulted in head injury.
Fallwell vs. Norpan Corp. (JJJ200),
consultant to attorney for defendant
concerning failure of gasoline pipeline.
McGaugh vs. McBride (JJK210), consultant
to insurer of owner of vehicle involved
in the failure of dump truck bed
hydraulic cylinder bracket.
Morris vs. CMI Corp., Twin City Hose, &
Viking Pump (JJK220), investigation for
attorneys for defendant of high
temperature failure of flexible
stainless steel asphalt transfer line.
Gary L. Brooks vs. Locke Supply Co.
(JJK230), investigation for attorneys
for defendant of failure of plastic
polymer water line fitting.
Pitco Frialators vs. Elmwood Sensors
(JJK240), consultant to attorney for
defendant concerning failure of
electrical switch in deep fryer.
Powell & Sons Trucking Hook/Block
Rebuild (JJL250), consultant to insurer
of trucking co. in shipping accident of
a block and hook rebuild.
Bend vs. Mobilel (JJL260), consultant to
attorney for defendant concerning
oil/gas piping failure in gas processing
plant.
White vs. WalMart (JJL270),
investigation for attorney of plaintiff
of failure and chipping of the head of
carpenter’s hammer.
Celsius vs. Atlas Tubular (JKA010),
consultant to attorney for defendant
concerning failure of casing in an
oil/gas well.
ALC Inc. Dump Truck Bed Failure
(JKA020), consultant to company
concerning weld failures in aluminum
truck beds.
Bryant vs. Purvis Bearing Services
(JKB030), consultant to attorney for
defendant of failure of bearing in
automated shelf-stocking equipment.
Arcadian vs. Schoeller Bleckmann
(JKB040), investigation for attorneys of
defendant of urea reaction explosion.
Mid-South Drilling of Jackson vs. Bowen
Tools & Homco (JKB050), investigation
for attorney for defendant of down-hole
failure of drill collar after failure of
drilling jar.
Stiles vs. Aluminum Service Corp.
(JKC060), consultant to attorney for
defendant concerning gaseous emission
from aluminum foundry.
Wind Shear Radar Dish, Will Rogers
Airport (JKC070), consultant to insurer
of assembler of wind shear radar dish.
Neal vs. Moss Planting & Arkansas Power
& Light (JKC080), consultant to attorney
for defendant concerning contact between
cotton module builder and electric line
pole resulting in electrocution of farm
worker.
1st Methodist vs. Whittaker, d/b/a
Quality Air (JKD090), consultant to
attorney for defendant concerning
furnace involved in fire.
Mitsubishi Accident (JKE100), consultant
to attorney for defendant concerning
fatigue failure of propeller hub on
Mitsubishi aircraft.
Guardiola vs. Davis & Winchester
(JKE110), consultant to attorney for
defendant concerning explosion of hand
gun.
Goff vs. Payless Cashways (JKF120),
consultant to attorney for defendant
concerning failure of pole barn nail
during extraction
Osborne vs. Ariens & Menco (JKF130),
consultant to attorney for plaintiff
concerning set spring failure on welded
riding lawnmower sulky.
Doyon Drilling Sling Failure (JKG140),
consultant to company on failure of oil
field tubular goods lifting sling.
Edwards vs. Cape Outfitters (JKH160),
consultant to attorney for defendant
concerning spontaneous discharge of an
over/under shotgun.
Garcia vs. John Deere (JKH170),
consultant to attorney for defendant
concerning sheet metal pullout failure
and pickup rigging of cotton picker.
Davis vs. Sloan (JKI180), consultant to
attorney for defendant concerning piping
failure resulting in propane
fire/explosion.
Porter vs. Primeco & M.H.E.E.I.
(JKI190), consultant to attorney for
defendant concerning failure of welds in
scissor jack man lift.
Perkins, et al vs. Air Liquide (JKI200),
investigation of explosion and fire in
oxygen pumping station as the result of
improper straining of welding debris
from pipeline.
TMJ Device Failure (JKI210)
investigation of failure of stainless
steel jaw implant device used to
reposition jaw.
McGee vs. Elmwood Sensors (JKJ220),
consultant to attorney for defendant
of failure of an electrical switch in a
deep fryer resulting in a fire.
Cline Truck Accident (JKJ230),
consultant to attorney for defendant
concerning chain and pole weld failure
in truck/automobile accident.
Dallas Hermetic Air Conditioning Crank
Shaft Failure (JKK240), consultant to
air conditioner compressor rebuilders of
fatigue failure of crankshaft.
Nowell vs. Ford (JKK250), consultant to
attorney for plaintiff regarding weld
failure on brake pedal leading to
automobile accident.
Boxberger Knodt Rods (JKK260),
consultant to attorney for plaintiff
regarding failure of Knodt rod spinal
implant failure.
Baugus vs. Bizmart (JKK270), consultant
to attorney for plaintiff concerning a
defectively welded chair leg.
Rakes vs. Simon R.O. Corp. (JKK280),
investigation for attorney for defendant
of failure of weld on pole digger
pedestal.
Meza vs. Dana/Wilson Wichita (JKL290),
consultant to attorney for defendant
concerning drilling rig collapse.
Eskite vs. Channel Home Centers
(JKL300), consultant to attorney for
defendant concerning articulating ladder
failure.
Dykes vs. Jackson Gas and Oil (JIE100
and JMB040), consultant to attorney for
defendant concerning failure of propane
gas heater connection.
Perkins vs. Air Liquide (JKI200),
consultant to attorney for defendant of
flash fire burn through stainless steel
pipeline in oxygen letdown station.
Botts vs. Alumax Aluminum (JLA010),
investigation for attorney for defendant
of aluminum corrosion from emission of
gaseous smoke.
Fuentes & Seigiera vs. McGuire
Industries, et al (JLB020) investigation
for attorney for defendant of failure of
oil field equipment.
Daniel Irvin vs. Springfield, Inc.
(JLB040), investigation for attorney for
plaintiff of shotgun discharge.
Michael Langston vs. Phillips Petroleum
(JLB050), investigation for attorney for
defendant of failure of vehicle axle
resulting in van rollover.
Air Liquide Pigtail Incident (JLB060),
investigation of debris after oxygen
incident in gas manifold at gas plant
explosion.
Rim Ring Failure (JLB070), investigation
for attorney for plaintiff of failure of
rim of mounted tire which exploded.
Lankford vs. Torch Energy (JLC080),
investigation for attorneys for
plaintiff to determine cause of
explosion of natural gas compressor
engine.
Gilchrist vs. Fontaine (JLD090),
investigation for attorney for plaintiff
of alleged failure of ladder.
Davis Crane Failure/Joe Mangan Tree
Service (JLD100), evaluation of crane
collapse and outriggers boom which
struck residence.
Sherry vs. Wellmark & Natco (JLD120),
investigation for attorney for defendant
of failure of fitting on oil field
pressure vessel during hydro testing.
Boyles Galavanizing Co. vs. Protherm
Engineering Ltd., Protherm, Inc. and
Munich Welding, Inc. (JLE130),
consultant to attorney for defendant
regarding failure of zinc plating
galvanizing kettle tank.
Hugh Porter vs. Majestic Co. & Eastbrook
Builders (JLE140), investigation for
attorney of defendant of metallurgical
evidence in chimney fire.
Chair Failure (JLF170), investigation of
failure of bowling alley chair at braze
repair in chair leg.
Xylene Drum Explosion (JLH180),
evaluation of explosion of 55 gallon
drum containing residual xylene.
Miller vs. Mid-Continent Aircraft
(JLH190), consultant to attorney for
defendant of failure of left main gear
on Cessna 421B aircraftupon landing.
Schrauth Ladder Failure (JLH200),
consultant to attorney for plaintiff of
failure of fire truck aerial extension
ladder during training exercise.
What-a-Burger vs. Pitco (JLI210),
consultant to attorney for defendant of
fire which originated at deep-fry unit
of house fan bracket failure.
Deere & Co. vs. Prince Manufacturing
(JLI220), investigation for attorneys
for plaintiff of failure of hydraulic
cylinder.
IHP vs. AECC (JLI230), examination of
corrosion of power plant piping for
attorney for plaintiff.
Lockett Towed Vehicle Release (JLI240),
investigation for attorney for plaintiff
of failure of release of towed vehicle
from tilt bed truck
Estate of Blanc Cancio vs. Hyundi Motors
(JLI250), consultant to attorney for
plaintiff regarding collision involving
Hyundi automobile.
Doyon Drilling Pipe Corrosion (JLJ260),
evaluation of pitting corrosion on drill
pipe in mud pit on north Slope.
Reaves vs. Deer Me Products (JLJ270),
investigation of failure of tree step.
Carolyn Tigert vs. Osteomed (JLJ280),
investigation for attorney for plaintiff
of failed TMJ device.
Leg Implant Device Failure (JLK290),
investigation for attorney for plaintiff
of failure of stainless steel nail leg
implant.
Maria Ovieda vs. Austin Coca-Cola
Bottling Co., Inc. (JLK300), consultant
to attorney for defendant of failure of
sight glass in pressurized container.
David Lovvorn vs. Krauss Lighting &
Maxim Lighting (JLK310), investigation
attorney for plaintiff of chain failure
causing chandelier to fall.
City of Lubbock vs. Steam Specialties
(JLL320), examination for attorney for
defendant of failure of thrust
plate/thrust bearing.
Ladder Inspection (JMA020), examination
of failed ladder for attorney.
Fan Hanger Bracket Failure (JMA030),
examination for attorney for
plaintiff of house fan bracket failure.
Sherri Evjen vs. Synthes (JMB030),
investigation for attorney for plaintiff
of fatigue failure of TMJ device.
Gerald Bohall vs. Steve Mahaffey
Construction, Inc. & Archer Daniels
Midland Co. (JMC050), investigation of
corrosion failure of roofing in
feed/grain processing plant which
resulted in workman falling through
corroded roof.
Kirby vs. Patterson Energy (JME060),
investigation for attorney for defendant
of oilfield drilling rig collapse.
Lawson Petroleum vs. Exxon Corp.
(JME070), consultant to attorney for
defendant of corrosion of casing strings
and salt water.
Keller Step Ladder Failure (JME080),
investigation for attorney for plaintiff
of failure of aluminum stepladder
supported on uneven sidewalk.
Intel vs. DKD Electrical Contractors
(JME090), investigation for attorney for
defendant of electric wire abrasion and
arcing inside electrical conduit.
Deaf Smith Co. Grain Processor vs.
Springer Electric Coop (JMF100),
investigation for attorney for plaintiff
of wire splice failure and high voltage
fire.
Petra Chemical Co. Chlorine Spill
(JMF110), evaluation of corrosion
resulting from chlorine spill.
Mosley Well Service, Inc. vs. Armco,
Inc. (JMG120), investigation of failure
of drilling rig line anchor.
Natkin Cap Screw Failure (JMH130),
investigation of failure of screws in
evaporative cooler.
Tradler vs. Pengo, C&L Aluminum Foundry,
Inc. (JMI140), consultant to attorney
for defendant of failure of aluminum
casting and insulator string.
Mosoyoni vs. U.S. Can (JMI150),
investigation for attorney for plaintiff
of aerosol can explosion.
Battery Hold Down Bracket (JMI160),
investigation of failure of aluminum
battery hold-down bracket which resulted
in electrocution and fire.
Elias vs. Swanson Auto Repair (JMJ170),
investigation for attorney for plaintiff
of automobile frame straightening
machine lift (jack) failure.
Hornsby vs. SPS (JMJ180), evaluation of
role of electrical arcing in range fire.
Tolbert vs. SPS (JMJ190), investigation
of failure of attachment line to house
as result of wind-induced metal fatigue.
Brandon Gray vs. Affiliated Foods
(JMK200), evaluation of conditions of
head light-post accident for attorney
for defendant.
McDiffet vs. McCollough (JMK220),
evaluation of failure of step ladder.
AC/DC Partnership vs. Ohio Casualty Ins.
(JML230); investigation for plaintiff of
corrosion from chlorine spill, and
hydrochloric acid formation.
TU Electric vs. F & E Erection (JNA010),
investigation for attorney for plaintiff
of failure of dewatering bin.
Spencer vs. Selfix & Dynacast (JNB020),
investigation for attorney for plaintiff
of failure of swag hook which caused
hammock to fall.
Louviere vs. Action, Inc., d/b/a Horse
and Rider (JNC030), investigation of
horse bit casting failure.
Donna Fletcher vs. Allsteel, Inc,
(JNC040) evaluation for attorney for
defendant of failure of office chair.
Sage Signs vs. Amarillo Thermo King,
Inc. (JNC050), investigation of wheel
failure on truck.
Lopez vs. Wescon & Delwood Foods,
(JNC060), investigation for attorney for
defendant of failure of tire rim on
truck.
Kose vs. Cablevision (JNC070),
investigation of dropping of cablevision
line on to roadway creating hazard for
motorcycle operator.
Duncan Properties Tubing Corrosion
(JNC080), investigation of down-hole
corrosion failure of tubing in McMakin
#1, Washita County, OK.
Blanton vs. Flintlock (JND100),
examination for attorney for plaintiff
of candle making ladder failure.
Cabrera Grinder Shaft Failure (JND120),
examination of failed grinder shaft.
Lubbock Commercial Bldg. vs. Maxine’s
Accents, Inc. (JNE130), investigation
for attorney for defendant of arcing
failure of electrical appliance wire.
Honeycutt vs. Neighbors (JNE140),
investigation for attorney for
plaintiff of failure of copper water
pipe.
Vacuum System Acid Damage (JNE150),
investigation for chip manufacturer of
acid damage to commercial chip-making
vacuum chambers.
KN Pipeline Rupture (JNE160), assessment
of cause of pipeline failure.
Sandovall vs. Discount Tire Co.
(JNE170), examination of truck wheel lug
failure in wheel and tire accident.
Daryan vs. Rheem Mfg. (JNE180),
investigation for insurer concerning
leak of residential water heater plastic
(polymer) valve.
Ice Group Addison vs. C.W. Davis Supply,
Chill-Con Products, Ltd. (JNE190),
investigation of corrosion failure of
heat exchanger tubes.
Butler vs. Eastern Maine Medical Center
(JNE200), analysis of fractured
prosthesis for attorney for defendant.
Teague vs. Joint Medical Products
(JNE210), evaluation of failed hip joint
implant.
Wendell Farley vs. Akron Brass (JNF220),
investigation for attorney for plaintiff
of failure of fire hose adapter.
Josefina Vasquez,vs. Austin Commercial,
Inc. (JNH230), investigation for
attorney for plaintiff of wire rope
failure resulting in construction crane
boom collapse.
Pautsky vs. Enserch Exploration
(JNH240), investigation and evaluation
for attorney for defendant of rust
buildup on valve body.
Aluminum Hub Towers East (JNH250),
examination for consultant C. Rogers of
cracking of aluminum fan hub.
Danals Food Stores Inc. vs. Valmont
Electric (JNI260), evaluation of fire.
Camilla Haynes vs. Culpepper
Enterprises, Inc. (JNI270),
investigation for attorney for defendant
of failure of highway grass mower blade
which resulted in fatality.
Water Sprinkler Pipe Leak (JNI290),
consultant to attorney for defendant of
water sprinkler piping failure resulting
in damage to stored pecan crop.
Delta Dailyfoods Texas, Inc./Automated
Ice, Inc. (JNJ300), investigation of
fractured weld on evaporative cooler.
Bolt Failure Analysis (JNJ320),
investigation of failure of aircraft
bolt.
Perkins vs. Entergy Corp. (JNK310),
investigation for attorney for defendant
of failure, fire of hydrogen gas
pipeline and valve assembly.
Castrellon vs. Villas at Turtle Creek
(JNK330), investigation for attorneys
for plaintiff of failure of scaffolding
support.
Estate of Allen vs. TCA Cable (JNK340),
investigation of dislodged hardware in
which logging truck load struck low
cable and caused fatality.
Panhandle Trucking vs. Dave Roberts
Leasing (JOA010), inspection for
attorney for plaintiff of truck steering
gear failure
Richard A. McDonald vs. Oilfield Pro Log
Services, Inc. (JOA020), evaluation for
attorney for plaintiff' of oil well
metal and tool samples.
Wicker 1998 Western Star Fire (JOA030),
investigation of burned tractor.
Stephens & Johnson Operating Co., Inc.
vs. C & H Pipe Rental & Supply Co., Inc.
(JOA040), investigation for attorney for
plaintiff of failure of down-hole tubing
during acidization of well which
resulted in question about tubing grade.
Gonzales vs. Rosa’s Café (JOA050),
investigation of explosion of cast
aluminum pressure cooker.
Arto Saw Blade Tip Failure (JOB060),
investigation for attorney for plaintiff
of failure of brazed carbide tip on
Credo 10" circular saw blade.
Joyce vs. Raleigh USA (JOC070),
investigation for attorney for defendant
of failure of welded bicycle frame
tubing connection.
Tony Smoker Injury (JOC080),
investigation for attorney for
plaintiff of failure of a racking board
component.
Wilkinsons vs. J.P. Ward, et al
(JOC090), investigation of a gas “T”
joint.
Nelson vs. Synthes, Inc., (JOD100),
investigation for attorney for plaintiff
of the failure of titanium spinal fusion
plate.
Ava Greene Johnson, et al vs. Shell
Offshore (JOE110), investigation for
attorney for plaintiff of failure of
wire rope.
Mills vs. Sherwin Williams Co. (JOE120),
investigation for attorney for
defendant of failure of paint can.
Lindell vs. Giant Bicycle (JOE130),
investigation for attorney for defendant
of bicycle seat bolt failure.
Endsley vs. Commercial Door Co. of
Dallas, Inc. (JOE140), investigation for
attorney for plaintiff of failure of
overhead door spring on overhead door at
American Airlines at DFW Airport.
Bridger Oil vs. Boyd Well Service
(JOE150), investigation for
plaintiff of failure of well rod string.
Olympic Pipeline vs. IMCO (JOH160),
accident investigation of gasoline
pipeline explosion.
U.S. Department of Labor vs. Austin
Commercial (JOJ170), continuation of
Vasquez vs. Austin (JNH230).
Campbell vs. Stanley Tools (JOJ180),
investigation for defendant of chipping
failure of hammer.
Fire Extinguisher Failure (JOJ190),
investigation for plaintiff of fire
extinguisher failure.
Stephanie Milan vs. Don DeCristo
Concrete (JOJ200), investigation for
attorney for defendant of failure of
brace on slab section at building site.
Union Pacific Warika Derailment
(JOK210), evaluation of metallurgical
evidence resulting from train
derailment.
Glascock vs. Pocahontas Ford & Mercury
(JOK220), investigation for defendant
attorney of failure of auto wheel studs
and loss of wheels.
Cameron vs. Harper Trucks Inc. and
Wal-Mart Stores, Inc. d/b/a Sam’s Club,
(JOK230), investigation of cart wheel
failure while inflating.
Norbid Dickman vs. James Morris, Cooper
Indus. (JOK240), investigation for
attorney for plaintiff of fire caused by
arcing in a light fixture and thermal
protector.
Hernandez vs. Xcel Corp. and Panhandle
Forklift (JOK250), investigation for
attorney for defendant of battery lid
hinge failure.
Howell vs. Culbertson Stowers, Inc.
(JOL260), investigation for attorney for
defendant of failure of weld on
automobile axle housing.
Haynes and Giffin vs. Bush Hog, et al
(JOL270), investigation for attorney for
plaintiff of failure of Bush Hog mower
blade.
Genesis Crude Oil Pipeline Failure
(JOL280), investigation of failure of
crude oil pipeline.
Mansure vs. Hicks (JOL290),
investigation for attorney of fire
presumed to have electrical initiation.
U. S. Army Pine Bluff Arsenal Flange
Failure (JPA010), investigation of
failure of flange carrying white
phosphorus.
Farrell Boating Accident (JPA020),
investigation of boating accident which
resulted in fatality.
Unique Functional Products Spring
Failure (JPA030), evaluation of failure
of brittle trailer spring.
Four Vehicle Accident/Trailer Wheel
(JPA040), evaluation of tractor trailer
wheel disengagement which resulted in
four vehicle accident.
Crane Wire Rope Failure (JPA050),
investigation of construction crane wire
rope failure.
West Coast Liquidators vs. Broadmoor
(JPA060), metallurgical evaluation of
failure of underground piping for fire
sprinkler system.
Malden Mills vs. Rhone-Poulene (JPB070),
investigation for attorney for defendant
of pipe and boiler components in textile
mill fire.
Buckley vs. Allied Products Corp.
(JRE020), investigation for attorney for
plaintiff of a Bush Hog mower blade.
Reyes vs. Quality Iron Works (JRE030),
evaluation of chipping from machine shop
press die.
Mendoza vs. Watson/Hopper, Inc.
(JRJ040), investigation for defendant of
racking board pin deformation and
drilling rig collapse.
Maine Fire Truck Fitting (JSA010),
investigation of brass high pressure
fitting failure and fatality.
John Soules Food Pipe Failure (JSA020),
investigation of steel pipe
fracture/failure from a low vacuum
ammonia system.
McLeon vs. Vulcan Materials (JSA030),
metallurgical failure analysis of
corroded pipe nipple which failed and
allowed chemical release.
Rost Litigation (JSA040), investigation
for attorney for defendant of failure of
a truck wheel axle and collision of
wheel with vehicle.
Gary Henson vs. Northern Pipeline
Construction Co. (JSB050), investigation
of failure of wheel studs on truck tire
resulting in wheel striking plaintiff.
Beck Plumbing Leak (JSB060),
investigation of copper water pipe
corrosion and electrical arcing.
Perot Systems Entrance Gate Swing Pins
(JSB070), investigation of fatigue
failure of hinge pins for electronic
entrance gate.
Leyva vs. TXU (JSC080), metallurgical
evaluation of pipeline corrosion of
natural gas distribution of pipe
allowing gas to migrate into water line.
Julian & Amber DeMine vs. Panhandle
Steel Erectors, et al (JSD100),
investigation of failure of slewing gear
on crane during lift which resulted in
personal injury. Slewing gear was found
to have metallurgical defects from
improper heat treatment. Positioning of
the slewing gear during crane
manufacture was also defective.
Howard vs. J & W Corp (JSE110),
investigation of failure of wheel lugs
on tractor trailer wheels resulting in
separation of dual wheels from vehicle
which then collided with passenger car.
Auto Wheel Failure (JSF120),
metallurgical evaluation of failed
aluminum wheel resulting in automobile
rollover.
Bobby Joe King, Marks Crane & Rigging
vs. Threldkeld (JSG130), metallurgical
investigation of failure of crane bolts
associated with slewing gear failure.
Hughes SUV Accident (JSG140),
investigation for attorney for plaintiff
of multi-truck collision involving 4
wheel drive u-joint, ball joint and
wheel failure.
1998 Ford Expedition Axle Failure
(JSH150), metallurgical evaluation of
Ford Expedition rear axle and the
contribution of the failure to one
vehicle accident.
Clinker Cooler Shaft Failure (JSH160),
metallurgical evaluation of clinker
cooler shaft as a result of
design/manufacturing defect.
Coleman vs. Dunn Roadbuilders (JSI170),
investigation for attorney for defendant
of failure of wheel lugs.
Ibarra vs. Rexcon Industries (JSI180),
metallurgical failure analysis of high
pressure hydraulic fitting on road
paving equipment.
Blair vs. Sam’s Club East, Inc.
(JSI190), investigation of failure of
lawn chair for attorney for plaintiff.
Marotta Wheel Accident (JSJ200)
investigation of right rear dual wheels
separation from tractor trailer while
traveling on highway resulting in
injuries. Failure due to welding on
wheel rim.
DynMcDermott 316 Sensitization
Investigation (JSK210), determination of
possible sensitization of valve
materials.
Walters vs. Trail King (JSK220),
investigation for attorney for plaintiff
of trailer pin failure while loading
equipment on loading ramp.
Gryphon Exploration vs. Cliff’s
Drillings (JSK230), investigation for
attorney for plaintiff of failure of 2
7/8 inch P-110 couplings/collars.
Litloff vs. Click’s Billiards (JSL240),
investigation of motorcycle collision
and the involvement of bungee cord
wrapped around wheel.
Forklift Boom Bolts Failure (JTA010),
investigation for attorney for plaintiff
of failure of bolts and frame structure
on forklift after collision with bridge.
Clulee vs. Belmont Homes (JTA020),
investigation for attorney for plaintiff
of failure of valve retainer nut in
kitchen water faucet which caused leak.
Ulrich vs. ATC/Vancom (JTA030),
investigation for attorney for defendant
of failure of bus door components.
Terry Brimer Accident (JTA040),
investigation for attorney for plaintiff
of failure of stair railing resulting in
fatality.
Martinez vs. Deere & Co. (JTB050),
metallurgical evaluation of farm tractor
seat.
Farr vs. Cottrel, Inc. (JTB060),
investigation of failure of load bender
chain used to hold automobile in place
during highway transportation.
Bryant Doiron Stool Failure (JTB070),
investigation for attorney for plaintiff
of failure of 24” stool that collapsed
and caused injury.
Jackson vs. Phillips Machine (JTC080),
metallurgical failure analysis and
accident investigation of coal mining
shuttle car canopy leg failure.
Bridges vs. Hydra Rig/Varco (JTC090),
investigation of a failed stripper bowl
adapter plug in oilfield snubbing unit
resulting in fatality.
Estep vs. Trans-Matic Mfg. Co. (JTC100),
consultant to attorney for defendant in
evaluation of spot-weld failure in a
line trimmer clutch.
Ortega vs. General Tool, Inc. (JTC110),
investigation for attorney for defendant
of diamond tipped saw blade.
Mendoza vs. Howell Equipment Co., Inc.
(JTC120), investigation for attorney for
plaintiff of swing set S hook failure
resulting in injury to child.
CMD Realty Water Line Failure (JTC130),
investigation of corrosion of 10 inch
cooling water line.
The Hartford vs. NIBCO, Inc. (JTC140)
investigation for attorney for defendant
of hot water valve failure due to
improper valve installation.
Rhoudes vs. Watts Treating Chemicals,
Inc. (JTE150), investigation of failure
of 600 psi ball valve during hot oil
treatment.
Burtchett vs. Cedar Fair (JTE160),
examination of failure of bolts on base
of amusement park ride.
Roof Panel Hail Damage (JTE170),
metallurgical evaluation of damage to
Duralum steel roofing from extreme hail.
Sayre vs. Avenger Chassis (JTE180),
investigation for attorney for plaintiff
of sprint car roll cage failure.
Reynolds vs. Massey (JTE190), analysis
of fitting failure on steam coal mining
equipment.
Failure of Boat Ladder (JTF200),
investigation of boat ladder failure.
Bucci vs. Roderick Clemente, M.D.
(JTF210), investigation for attorney for
defendant of stainless steel osteotome
blade failure during surgery.
Porras Accident Investigation (JTF220),
investigation of F-150 Ford truck wheel
axle failure.
Katty vs. WTG (JTF230), investigation of
natural gas compressor failure resulting
in explosion of natural gas pumping
station.
Ayre vs. Toastmaster (JTF240),
metallurgical evaluation of a kitchen
toaster switch failure and its relation
to a house fire.
Offshore Platform Ladder Failure
(JTG250), metallurgical evaluation of
offshore platform ladder failure.
Gary Swindle vs. The HON Co. (JTG260),
investigation for attorney for plaintiff
of failure of re-welded HON office
chair.
Sidener vs. Little Giant Ladder
(JTG270), metallurgical evaluation and
failure analysis of hinge failure in an
articulating ladder.
O’Dell vs. Ryobi (JTG280), failure
analysis of carbide teeth which failed
on circular saw resulting in eye injury.
Safety Line Snap Hook Failure (JTH290),
examination of safety line snap hook
that failed.
Diamond Shamrock vs. Puffer-Sweiven
(JTI310), investigation for attorney of
failed valve causing rupture and
explosion at Three Rivers Refinery.
Mona Tea Kettle (JTI340), investigation
for attorney for defendant of lead in
tea kettle.
Jerry Mitchell Boat Hook Failure
(JTI350), investigation for attorney of
defendant of failure of boat hook with
tow-rope and tube.
Garza, et al & Carlos Figueroa, et al
vs. United Resources (JTJ370), weld
failure evaluation of improperly
constructed sump tank that exploded
during pressurization at an oil and gas
well site by workers.
Taylor/Bergeron vs. Mark’s Backhoe
Service (JTK380), evaluation of cause of
leakage in 12” gate valve which resulted
in gas explosion and refinery fire.
Ruiz vs. Valley Welding Service
(JTK400), metallurgical failure analysis
of trash bin gate hinge failure.
Spencer vs. Maverick Tube Corp.
(JTK410), investigation for attorney for
defendant of oilfield casing failure.
Olsen-Beal Association Wind Farm
(JUA010), investigation for defendant of
failure of wind generator turbine shaft.
Palmer vs. Ledwell & Sons (JUA020)
inspection of truck ladder which failed
as a result of improper usage.
Sharp vs. Altec Industries, Inc.
(JUB030), investigation for attorney for
plaintiff of failure of bucket truck
bucket components and hydraulic
cylinder.
Ritz Carlton Construction Project
(JUB040), evaluation of possible
corrosion damage as a result of
Hurricane Ivan at Ritz Carlton
construction site in Grand Cayman,
Cayman Islands.
Powell vs. Harper Trucks (JUB050),
investigation for attorney for defendant
of failure of wheel on two wheel cart
after inflation.
Morgan vs. Melbourne Hospitality
Associates (JUC060), investigation for
attorney of defendant of malfunctioning
hotel elevator.
Moore vs. JFK Medical Center (JUC070),
failure analysis of surgical instrument
resulting in fragment being left in
patient’s sinus.
Welded Stair Failure (JUD100),
investigation for plaintiff of
welding defects of wire rope hand rails
used in temporary handrail attachment.
Pioneer Natural Resources, Inc. vs. Coma
Well Service, Inc., (JUE110),
investigation for attorney for defendant
of failure of oilfield tubing line wire
rope.
Teweles Copper Pipe (JUE120),
metallurgical evaluation of copper pipe
from rural residence.
Edmonson vs. Tree City Tool &
Engineering (JUE130), investigation for
attorney for defendant of failure of
automatic welder door mechanism that
resulted in door falling and hitting
operator.
Fontneot vs. Dodson Aviation (JUE140),
evaluation of horizontal stabilizer,
winglet failure on Bell helicopter.
Cindy Sawyer Ladder Failure (JUF150),
investigation for attorney for plaintiff
of step ladder failure.
Kunkel vs. Bluebonnet (JUF160),
investigation for attorney for plaintiff
of rear tractor trailer wheels detaching
and striking pedestrian.
Garwood vs. J & B Importers (JUG180),
evaluation of bungee cord hood failure.
Willbros Pipeline Failure (JUG190),
investigation of buckled pipeline
fracture in Nigeria, W. Africa following
terrorist attack.
Crane Collapse (JUG200), evaluation of a
collapsed crane that resulted in damage
to residence.
Taylor vs. Woolley Tool (JUH210),
evaluation of failure of oilfield
mechanical tong tool containing casting
flaw.
Carney vs. NIBCO (JUH220), investigation
of failure of in-line gas valve failure
during fire.
Morbark Tub Grinder Failure (JUJ230),
investigation for insurer of failure of
tub grinder used for grinding trees and
brush.
Flippin vs. Crocker Crane (JUJ240),
investigation of failure of chain link
in “come-along” which resulted in
derrick sliding inside a water tower
under construction. Derrick fell
resulting in impact failure of derrick
section attachment bolts.
NUCONSTEEL Shaft Analysis (JUJ260),
evaluation of failed shaft fracture
surface with high stress concentration
due to rotational bending fatigue.
CAT 322 Excavator (JUK270),
investigation for insurance carrier of
effect of electrical current from power
line which struck CAT 322 excavator
causing electrical arcing damage
throughout.
Hopper vs. Stahlman Plumbing (JUK290),
investigation of failure of residential
gas line leading to newly installed
floor furnace.
Bonita Springs Fire Control & Rescue
Fire Station No. 4 (JUL300),
investigation for plaintiff of the
effect of muriatic acid on newly
constructed fire station.
Water Leak at Hampton Inn and Suites
Fort Worth, Texas (JUL310),
investigation for insurance carrier of a
CPVC sprinkler pipe which caused water
leak at Hampton Inn and Suites, Fort
Worth, Texas.
Water Leak at Agape Fellowship (JUL320),
evaluation of a water line elbow failure
resulting in internal ice formation.
Christensen Sunfire Pontiac Accident
(JVA010), investigation for attorney for
plaintiff of separation of front and
rear doors of automobile during low
speed accident.
Furnace Auger Material ID (JVC020),
examination of failure of furnace augers
as result of casting defects.
Caldwell vs. Baptist Hospital (JVC030),
evaluation of titanium screen used
during cranial surgery.
Lindy Lott Wrecker Service, Inc.
(JVC040), investigation for insurance
carrier of the failure of bus axle.
Hardt Water Heater Pipe Evaluation
(JVC050), evaluation of failure of 3
year old water line.
Astro World, L.P. vs. Louis Crane &
Hoist (JVC060), investigation for
attorney for defendant of damage to
“Batman Escapes” ride during teardown
and removal.
Claudia Rivas vs. Rolling Stones, Inc.
(JVC070) evaluation of truck axle
failure causing trailer wheels to exit
rock hauling trailer.
Lara Single Vehicle Accident (JVD080)
investigation of wheel and axle failure
in single vehicle accident resulting in
fatality.
Trailer Door Spring Failure (JVD090),
investigation for insurer of trailer
door spring failure causing amputation.
Ford Explorer Wheel Loss (JVE100),
examination of wheel separation
resulting in rollover of vehicle.
Truck Service of LA (JVE110),
investigation of corrosion and defective
weld repair which resulted in failure of
trailer hydraulic system during dumping
operation.
Cast Iron Milling Machine Crack
(JVE120), evaluation of cast iron
milling machine fracture and base
failure.
Fuel Nozzle Clip Evaluation (JVF130),
investigation of fuel nozzle clip
failure as result of stress corrosion
cracking from improper material
selection.
Mega vs. Towbin Dodge (JVG140),
investigation of cotter pin failure
which caused wheel to exit from vehicle
resulting in loss of control.
Airgas Propylene Tank (JVG150),
evaluation of integrity of propylene
cylinders (LX or 4BA240) under full sun
conditions.
Powell vs. M & W Hot Oil, Inc. (JVH160),
investigation of ball valve leak during
oilfield hot oiling operation.
Harendt vs. Basic Energy Services
(JVH170), investigation of wellhead
nipple that failed and blew off and
resulted in injury.
Boudreaux vs. Louisville Ladders
(JVH180), investigation for plaintiff of
failure of ladder.
Johnson vs. Federal Express (JVI190),
investigation for defendant of
alleged loose steering components and
their role in one vehicle tractor
trailer accident.
Stanley Screwdriver Analysis (JVI200),
investigation of screwdriver which
failed in bending while being improperly
used.
Dennis vs. Furniture Factory Warehouse
(JVJ210), evaluation for attorney for
plaintiff of defectively welded
swiveling bar stool which failed during
use at retail location.
Jackson & Simmen vs. Texas Specialty
Trailers, Inc. (JVJ220), investigation
for defendant of alleged weld
failures and their role in a one vehicle
oilfield accident.
Harmon Tank Rupture (JVJ230),
metallurgical evaluation of fuel tanker
that exploded due to hydrogen
blistering.
Lexington vs. Kellogg (JVK240),
investigation of failure of casting
defects in plant process motor.
Tractor Homicide Investigation (JVK250),
evaluation of physical damage of two
tractors during collision.
Jeffery Byram Motorcycle Accident
(JVL260), investigation for attorney for
plaintiff of failure of motorcycle frame
involved in accident.
Charmane Jackson vs. U.S. Kids Golf,
investigation for attorney for plaintiff
of failure of kid’s golf club shaft
resulting in fatality.
Thompson vs. Dixon & Tulane University
(JVL280), investigation for plaintiff of
failure wrist plate implant.
Hopper vs. Equitable Gas & Stahlman
Plumbing & Heating (JVK290)
investigation of house explosion
purported to have initiated from defect
in furnace installation.
Sanchez vs. Interdynamics, Inc.
(JWA010), investigation for attorney for
plaintiff of failure of Freon can during
filling of automobile air conditioner.
O’Brien vs. H2O Fires System (JWA020),
investigation of over-torqued bolt
failure on sprinkler system coupling.
LaLonde Motorcycle Accident (JWB030),
evaluation of motorcycle front fork
shock absorber tube failure resulting in
loss of control.
Rival Crockpot Fire Investigation
(JWB040), evaluation of beads on
electrical wire believed to be arc
beads.
Stephen Lausen vs. ADP Plumbing
(JWB050), investigation for attorney for
defendant of fire involving release of
acetylene through vent plug.
Smiths Aerospace Components (JWC060),
evaluation of failure of EB welding on
jet engine diffusers.
Judith Miller vs. Armadillo Clay &
Supplies & Skutt Ceramic Products, Inc.
(JWD090), failure analysis of hinge on
lid of ceramic firing furnace.
Valero Refinery Explosion (JWD100),
investigation of a flange failure that
resulted in a propane/hydroflouric acid
explosion and fire.
Lanclos vs. Crown DBL, et al (JWE110),
failure analysis of oil field casing
lift sub.
Manfred Schweizer Turnbuckle Pin
(JWE120), investigation of failure of
turnbuckle allowing sailboat mast and
main sail to fall into ocean.
Daniel Akers vs. C&C Marine & Repair &
ABC Insurance Co. (JWE130),
investigation for plaintiff of failure
of Freon can during filling of air
conditioner.
XTO Energy Blowdown Pipe Failure
(JWE140), investigation of failure of
90° pipe elbow when gas blown was
attempted in gas processing plant.
Volvo Truck Hoe Boom Failure (JWE150),
evaluation of multiple cracking in
backhoe bucket used to off-load coal
from barges.
Holcim Gear Failure Evaluation (JWF160),
investigation of failure of gearbox gear
in cement grinding plant.
James Four Wheeler Accident (JWF180),
investigation for plaintiff of four
wheeler accident and the role of failed
aluminum casting.
Robert Cabell Accident (JWF190),
investigation for plaintiff of
cause/failure of tractor trailer flatbed
load loss.
Evaluation of 304L Stainless Steel
Corrosion (JWG200), evaluation of
corrosion on structural “I” beams in
food processing plant.
Tubing Grade Determination (JWG210),
determination of API tubing grade.
Highland Springs Pool Corrosion
(JWG220), investigation of
corrosion/tile staining around stainless
steel pool ladder/decking.
Thomas vs. MTS Seating (JWG230),
investigation for defendant of a chair
which failed as a result of two broken
welds.
Bruce vs. Mickey Truck Bodies, Inc.
(JWG240), investigation for plaintiff of
failure of truck air brake system.
Quirit vs. Vornado Air Circulation
(JWH260), investigation for defendant of
alleged electrical arcing in power cord
of electric fan.
Hawkins Construction Jackhammer Bit
(JWJ270), evaluation of fatigue fracture
of jackhammer bit.
Merriweather vs. Zig’s Building Supply
(JWF280), investigation for attorney for
defendant of failure of trailer hitch
tube resulting in horse trailer
detachment from towing vehicle.
Potlatch vs. Rubber Roller Co. (JWJ290),
investigation for defendant of repeated
failure of printing press ink roller
shaft ends.
Cressman Tubular vs. EBS Oil, et al
(JWK300), investigation for plaintiff of
failure of oil field tubular products.
TRX Casing Evaluation (JWL330),
evaluation for attorney for
plaintiff of repeated down hole casing
failures.
Scancilla vs. The Brickman Group
(JXB040), investigation for attorney for
defendant in failure of wheel bearing
resulting in tire colliding with another
vehicle.
Mary Arthur vs. Dometic Corp. and
Coachmen (JXB060), investigation for
attorney for defendant of failure of
refrigerator tubing and allegation that
tubing rupture initiated fire.
East Texas Medical Center Stainless
Steel Wire Failure (JXB070),
investigation for senior living facility
of stainless steel hangers holding up
ceiling panels.
Katrina Corrosion (JXB080), evaluation
of aging of corrosion on wall after
Hurricane Katrina.
Cano Petroleum Range Fire (JXC100),
investigation for attorney for plaintiff
of arcing/wear on downed lines and guy
wires involved in range fire.
Fields & Company vs. GEODynamics, Inc.
(JXD110), investigation for attorney for
defendant of oilfield tubing failures in
down hole perforating guns.
Lubbock County Prison Project (JXD120),
evaluation of internal corrosion of
hollow prison cell steel doors.
Chipper Jack Stand Failure (JXD130),
investigation for insurance carrier of
jack stand failure of mobile wood
chipper.
Copper Tubing/Joint Failure (JXD150),
investigation for defendant of failure
of copper tubing joint at Tulsa Bone and
Joint facility.
Rongeur Failure During Surgery (JXE160),
investigation for plaintiff of
failure of surgical rongeur.
Energico Petroleum vs. Tadlock Pipe and
Rental (JXF190), investigation for
attorney for defendant of tubing string
failure in Energico Petroleum well.
Rodkey Copper Water Pipe Corrosion
(JXF210), evaluation for insurance
carrier of external corrosion of water
pipe.
Cecil P. White vs. Dometic Corp.
(JXF220), investigation for attorney for
defendant of ammonia refrigeration
tubing and the relationship of tubing
perforation to initiation of a fire.
John Pierce vs. Rockwall Marine and
Teleflex Marine (JXF250), investigation
for attorney for plaintiff of failure of
bolts in outboard motor boat steering
control mechanism.
Boiler Vat Weld Failure (JXF270),
investigation for attorney for defendant
of failure of weld in pigskin boiler vat
resulting in fire.
Niagara Water Conveyor Link (JXH340),
evaluation of corrosion of newly
installed conveyor chain used for
cellophane wrapping of water bottles.
Wells vs. Lowe’s Home Center (JXI360),
investigation for attorney for defendant
of failure of tooth from circular saw
blade resulting in injury to user.
Pierce vs. Rockwell (JXF250),
investigation for plaintiff of cross
threading failure of boat tiller arm
attachment bracket,
State Farm/Helm (JXG300), investigation
for insurance carrier of corrosion
caused by electrical activity on copper
water pipe.
Thermodyn Contractors, Inc. vs. Tyco
Fire Products (JXG310), investigation
for attorney for defendant of failure of
copper fuse tube in sprinkler head cold
release.
Tadlock Pipe Evaluation (JXH350),
evaluation for plaintiff of
defective oilfield casing.
Zubia vs. Babcock Equipment Corp.
(JXK460), investigation for attorney for
defendant in matter concerning failure
of oilfield grab hook.
Tomaselli vs. Medinah Automotive
(JXK480), investigation for attorney for
plaintiff of accident involving 2006
Ford van.
Lexington Insurance vs. Menzer (JYA010),
investigation for attorney for
defendant of broken gas pipe connections
involved in gas leak which resulted in
explosion.
Willoughby vs. ACE European Group Ltd.
(JYA020), investigation for attorney for
defendant of failure of copper water
pipe.
Basa vs. Bourland and Leverich (JYB060),
investigation for attorney for plaintiff
of failure of P-110 tubing coupling in
gas well.
Fletcher vs. Woolsey (JYD090),
investigation for attorney for defendant
of motorcycle headlamp involved in two
vehicle accident.
Milan and Bustamante vs. Exline
(JYD100), investigation for attorney for
plaintiff of failure of wheel studs on
tire which exited a trailer resulting in
two fatalities.
Titeflex CSST (JYD120), investigation
for attorney for defendant of CSST in
Wilmington, Delaware.
Kerssemakers vs. Barry Reed Poteeet and
Metro-Tex Utilities Inc. (JYD130),
investigation for attorney for plaintiff
of object thrown by roadside mower.
Calhoun vs. Milstead Automotive
(JYE140), investigation for attorney for
defendant of failure of chain during
lifting of overloaded sea cargo
container.
Paul Robertson Rigging (JYE150),
investigation of failure of a sailboat
fitting on rigging while sailing off
coast of New Zealand.
Nationwide vs. Dometic (JYE160),
investigation for attorney for defendant
of fire allegedly caused by Dometic
refrigerator.
Brooks vs. Tanner Pipe (JYF180),
investigation for attorney for defendant
of failure of pin on a side boom
tractor.
Cox/GMAC vs. Dometic (JYF200),
investigation for attorney for defendant
of RV fire involving a Dometic
refrigerator in RV.
McNicoll vs. Northern Tool (JYG220),
investigation for attorney for plaintiff
of failure of split rim wheel from
garden crate wagon.
Community Coffee vs. Southern Automation
(JYH260), investigation for attorney for
defendant of coffee “super bag”
shelving.
Charles Gore Bicycle
Frame Failure (JZA020), investigation of
failure of bicycle frame
Newton vs. Moberg
Truck Services (JZF160), investigation
for attorney for defendant of failure of
wheel lugs and trailer wheel detachment.